Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cristal™ Renew 401-50 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Cristal™ Renew 401-50:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Cristal datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

Eastman Cristal™ Renew 401-50 copolyester is a high flow product that contains mold release for ease of ejection.

It is designed and engineered specifically for cosmetics packaging applications. With its unsurpassed color and

clarity and an unmatched ability to mold thick parts with improved gate aesthetics, Cristal 401-50 Renew is clearly

a well-suited copolyester for premium cosmetics packaging. Other outstanding features of Cristal™ Renew 401-50

copolyester are excellent chemical resistance, high gloss, and improvements in processing such as faster cycle

times, and lower scrap rates. Cristal Renew 401-50 is also ideally suited for two-shot molding techniques due to

its lower processing temperatures, very slow crystallization rate, and flow characteristics.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a

global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are

produced with ISCC certified circular content by mass balance allocation.


Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Ritiro di stampaggio, parallelo 0.0035 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2030 MPa ISO 527
Carico unitario a trazione 50 MPa ISO 527
Deformazione a snervamento 4.3 % ISO 527
Carico unitario a rottura 20 MPa ISO 527
Deformazione a rottura 39 % ISO 527
ASTM Data
Modulo a trazione 2036 MPa ASTM D 638
Resistenza alla trazione di snervamento 50 MPa ASTM D 638
Resistenza alla trazione a rottura 24 MPa ASTM D 638
Allungamento a snervamento 4.4 % ASTM D 638
Allungamento a rottura 44 % ASTM D 638
Modulo a flessione 1808 MPa ASTM D 790
Resistenza alla flessione 66 MPa ASTM D 790
Durezza Rockwell R 108 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 103 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 44 J/m ASTM D 256
Temperatura -40 °C -
Resistenza all'urto Izod, 1/8 in N J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
DTUL a 66 psi 68 °C ASTM D 648
DTUL a 264 psi 61 °C ASTM D 648
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 0.4 % ASTM D 1003
Trasmissione luminosa 91.8 % ASTM D 1003
Altre ProprietàValoreUnitáNorma del test
Densità 1280 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 65 °C -
Pre-essiccamento - Tempo 8 h -
Temperatura di fusione 205 - 240 °C -
Temperatura dello stampo 16 - 38 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Altre Estrusioni
Forma fisica disponibile
Colore naturale
Additivi
Agente di distacco
Caratteristiche speciali
Alto urto o modificato all'urto, Trasparente
Caratteristiche
High Gloss, Copolimero
Resistenza Chimica
Resistenza chimica generale
Certifications
ISCC Plus
Applicazioni
Imballaggio
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.