Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of DOWLEX™ 2645 - (PE-LLD) - The Dow Chemical Company

Material Data Center offers the following functions for DOWLEX™ 2645:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Dowlex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di Fluiditá, MFI 0.85 g/10min ISO 1133
Temperatura 190 °C -
Carico 2.16 kg -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Coeff.di dilatazione termica lin., parallelo 39 E-6/K ISO 11359-1/-2
ASTM Data
Temp.di rammollimento Vicat 107 °C ASTM D 1525
Proprietà OtticheValoreUnitáNorma del test
ISO Data
Opacità 10 - ISO 14782
ASTM Data
Brillantezza 59 - ASTM D 2457
Altre ProprietàValoreUnitáNorma del test
Densità 918 kg/m³ ASTM D 792
Proprietà Meccaniche (Film)ValoreUnitáNorma del test
ISO Data
Carico allo snervamento, parallelo 7.5 MPa ISO 527-3
Carico allo snervamento, normal 6.3 MPa ISO 527-3
Carico unitario a rottura, parallelo 39 MPa ISO 527-3
Carico unitario a rottura, perpend. 40 MPa ISO 527-3
Allungamento massimo, parallelo 560 % ISO 527-3
Allungamento massimo, perpend. 670 % ISO 527-3
Prova di caduta del dardo A 480 g ISO 7765-1
Tipo di estrusione blown - -
Spessore del provino 0.05 mm -
Caratteristiche
Processabilità e Forma di Forni
Estrusione di film in bolla, Estrusione Film
Forma fisica disponibile
Pellet, Bianco
Caratteristiche
Basso odore
Certifications
Contatto con gli alimenti, Approvato per l'utilizzo per contatto con alimenti 10/2011, Food contact notification (FCN)
Disponibilità geografica
Europa, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.