Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ EN001 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ EN001:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

Eastar™ EN001 Copolyester is a thermoplastic polyester copolymer and is suitable for food packaging applications.

Eastar™ EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming processes and helps maintain good clarity when processing much thicker sheet. Eastar™ EN001 copolyester can also be used for injection molding applications. It is the preferred general-purpose crystallizable PET for thermoforming.

Eastar™ EN001 copolyester is regulated for use in food packaging applications in accordance with US FDA Regulation 21 CFR 177.1315. It is lawful for use under US Department of Agriculture Food Safety Inspection Service regulations as a packaging material for meat or poultry food products prepared under federal inspection.




Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2400 MPa ISO 527
Carico unitario a trazione 57 MPa ISO 527
Carico unitario a rottura 25 MPa ISO 527
Deformazione a rottura 120 % ISO 527
Modulo a flessione, 23°C 2300 MPa ISO 178
Resistenza all'urto Izod, +23°C N kJ/m² ISO 180/1U
Resistenza all'urto Izod con intaglio, +23°C 4.5 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio 3.1 kJ/m² ISO 180/1A
Temperatura -40 °C -
Energia di perforazione, +23°C 15 J ISO 6603-2
Durezza Rockwell R 114 - ISO 2039-2
ASTM Data
Modulo a trazione 2400 MPa ASTM D 638
Resistenza alla trazione di snervamento 58 MPa ASTM D 638
Resistenza alla trazione a rottura 25 MPa ASTM D 638
Allungamento a rottura 120 % ASTM D 638
Modulo a flessione 2500 MPa ASTM D 790
Durezza Rockwell 112 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 40 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 27 J/m ASTM D 256
Temperatura -40 °C -
Resistenza all'urto Izod, 1/8 in N J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 65 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 69 °C ISO 75-1/-2
ASTM Data
DTUL a 66 psi 68.9 °C ASTM D 648
DTUL a 264 psi 65 °C ASTM D 648
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 1 % ASTM D 1003
Trasmissione luminosa 84 % ASTM D 1003
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1330 kg/m³ ISO 1183
Densità 1330 kg/m³ ASTM D 792
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Altre Estrusioni, Termoformatura
Caratteristiche
Copolimero
Certifications
Contatto con gli alimenti, Approvato per l'utilizzo per contatto con alimenti secondo la FDA 21 CFR
Applicazioni
Automotive, Imballaggio, Attrezzature sportive
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.