Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ EN067 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ EN067:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

Eastar™ Copolyester EN067 is a copolymer PET with good color. This product is supplied as a crystalline pellet that has improved flowability characteristics. Due to slower crystallization kinetics, this product is capable of producing a part free of crystalline haze upon injection molding. This product is tailored for the injection-molded cosmetics and personal care market.




Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Ritiro di stampaggio, parallelo 0.0035 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Resistenza alla trazione di snervamento 57 MPa ASTM D 638
Resistenza alla trazione a rottura 24 MPa ASTM D 638
Allungamento a snervamento 4 % ASTM D 638
Allungamento a rottura 134 % ASTM D 638
Modulo a flessione 2600 MPa ASTM D 790
Resistenza alla flessione 81 MPa ASTM D 790
Durezza Rockwell 110 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 58 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 29 J/m ASTM D 256
Temperatura -40 °C -
Resistenza all'urto Izod, 1/8 in N J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
DTUL a 66 psi 66 °C ASTM D 648
DTUL a 264 psi 61 °C ASTM D 648
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Trasmissione luminosa 84 % ASTM D 1003
Altre ProprietàValoreUnitáNorma del test
Densità 1320 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 150 - 160 °C -
Pre-essiccamento - Tempo 4 - 6 h -
Temperatura di fusione 270 - 290 °C -
Temperatura dello stampo 10 - 30 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Caratteristiche
Copolimero
Certifications
Contatto con gli alimenti
Applicazioni
Imballaggio
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.