Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Flomat 700/30 - UP-GF30 - Devi Polymers Private Limited

Material Data Center offers the following functions for Flomat 700/30:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Flomat datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
Other Standards[S]
Ritiro di stampaggio, parallelo 0.1 % BS-2782
S: These properties are reported by the producer according standards that are different to our defaults.
Proprietà MeccanicheValoreUnitáNorma del test
Other Standards[S]
Resistenza a trazione 78 MPa BS-2782
Resistenza alla flessione 118 MPa BS-2782
Resistenza a compressione 177 MPa BS-2782
S: These properties are reported by the producer according standards that are different to our defaults.
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
UL 94 combustibilitá V-0 - UL 94
Proprietà ElettricheValoreUnitáNorma del test
ASTM Data
Resistenza all’arco 185 s ASTM D 495
Other Standards[S]
Resistività volumica 1E11 Ohm*m DIN 53482
Resistività superficiale 1E12 Ohm DIN 53482
Rigidità dielettrica 10 kV/mm BS 2782
S: These properties are reported by the producer according standards that are different to our defaults.
Altre ProprietàValoreUnitáNorma del test
Other Standards[S]
Assorbimento d'acqua 0.2 % BS-2782
Massa volumica 1700 kg/m³ BS-2782
S: These properties are reported by the producer according standards that are different to our defaults.
Caratteristiche
Processabilità e Forma di Forni
Stampaggio a compressione
Forma fisica disponibile
Composti da stampaggio in lastra
Disponibilità geografica
Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.