Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of FORTRON® ICE 504L - PPS-GF40 - Celanese

Material Data Center offers the following functions for FORTRON® ICE 504L:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Fortron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

FORTRON ICE 504L is a 40% glass fiber reinforced polyphenylene sulfide, that belongs to our new generation of Fortron® PPS.
This new technology allows optimization of molding conditions with faster cycle times. Due to the faster crystallization of the material at a higher temperature, the option of mold wall temperature reduction can be subject of advanced process optimization. The potential for optimization of Fortron® ICE by cycle time reduction is possible by standard cavity surface temperatures of 140°C. The potential for lowering the mold temperature must be checked individually and it depends on process and part design.
 



Flammability @1.6mm nom. thickn.V-0-
Flammability at thickness h (0.38 mm)V-0-
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.3 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.6 % ISO 294-4, 2577
Capacità termica specifica del fuso 1500 J/(kg K) -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 15100 MPa ISO 527
Carico unitario a rottura 202 MPa ISO 527
Deformazione a rottura 1.9 % ISO 527
Resistenza all'urto Charpy, +23°C 53 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 53 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 10 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 10 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 280 °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 90 °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 270 °C ISO 75-1/-2
Temp.di inflessione sotto caricor, 8.00 MPa 215 °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 26 E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 42 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 class IEC 60695-11-10
Spessore provato 1.5 mm -
Reazione al fuoco a spessore h V-0 class IEC 60695-11-10
Spessore provato 0.4 mm -
Indice di ossigeno 47 % ISO 4589-1/-2
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 4.1 - IEC 62631-2-1
Fattore di dissipazione, 1MHz 20 E-4 IEC 62631-2-1
Resistività volumica >1E13 Ohm*m IEC 62631-3-1
Resistività superficiale >1E15 Ohm IEC 62631-3-2
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.02 % Sim. alla ISO 62
Massa volumica 1650 kg/m³ ISO 1183
Funzioni
Sforzi-deformazione , FORTRON® ICE 504L, PPS-GF40, Celanese
Modulo secante-deformazione , FORTRON® ICE 504L, PPS-GF40, Celanese
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Additivi
Agente di distacco
Certifications
Contatto con acqua potabile
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com