Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of FORTRON® 4184L6 DW - PPS-(MD+GF)53 - Celanese

Material Data Center offers the following functions for FORTRON® 4184L6 DW:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Fortron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Fortron 4184L6 is an easier flow version of Fortron 4184L4. for drinking water applications.  It offers similar characteristics to the 4184L4. This grade is especially used for thin walled parts requiring long flow lengths, stiffness and dimensional control. Applications made of this grade are typically electronic components.

Flammability @1.6mm nom. thickn.V-0-
Flammability at thickness h (0.75 mm)V-0-
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.3 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.6 % ISO 294-4, 2577
Capacità termica specifica del fuso 1500 J/(kg K) -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 16600 MPa ISO 527
Carico unitario a rottura 165 MPa ISO 527
Deformazione a rottura 1.4 % ISO 527
Resistenza all'urto Charpy, +23°C 29 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 29 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 7 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 7 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 280 °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 90 °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 270 °C ISO 75-1/-2
Temp.di inflessione sotto caricor, 8.00 MPa 215 °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 24 E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 32 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 class IEC 60695-11-10
Spessore provato 1.5 mm -
Reazione al fuoco a spessore h V-0 class IEC 60695-11-10
Spessore provato 0.8 mm -
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 4.7 - IEC 62631-2-1
Fattore di dissipazione, 1MHz 20 E-4 IEC 62631-2-1
Resistività volumica >1E13 Ohm*m IEC 62631-3-1
Resistività superficiale >1E15 Ohm IEC 62631-3-2
Rigidità dielettrica 27 kV/mm IEC 60243-1
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.02 % Sim. alla ISO 62
Massa volumica 1800 kg/m³ ISO 1183
Funzioni
Sforzi-deformazione , FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Modulo secante-deformazione , FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Sforzi-deformazioni (isocrona) 23°C, FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Modulo di scorrimento-tempo 23°C, FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Curva di scorrimento 23°C, FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Sforzi-deformazioni (isocrona) 120°C, FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Modulo di scorrimento-tempo 120°C, FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Curva di scorrimento 120°C, FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Sforzi-deformazioni (isocrona) 150°C, FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Modulo di scorrimento-tempo 150°C, FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Curva di scorrimento 150°C, FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Sforzi-deformazioni (isocrona) 200°C, FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Modulo di scorrimento-tempo 200°C, FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Curva di scorrimento 200°C, FORTRON® 4184L6 DW, PPS-(MD+GF)53, Celanese
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Additivi
Agente di distacco
Caratteristiche speciali
Stabilizzato o stabile alla luce, Stabilizzato o stabile al calore
Altre informazioni
Stampaggio ad Iniezione
Predrying in a dehumidified air dryer at 130 - 140 degC/3-4 hours is recommended.
On injection molding machines with 15-25 D long three-section screws, as are usual in the trade, the FORTRON is processable. A shut-off nozzle is preferred to a free-flow nozzle.

Melt temperature 320-340 degC
Mold wall temperature at least 140 degC

A medium injection rate is normally preferred. All mold cavities must be effectively vented.
Tool temperature of at least 135 degC is recommended for parts to achieve maximum crystallizable potential.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.