Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KOPLA® KNL1040 - PA6-GF40 - KOPLA CO., LTD

Material Data Center offers the following functions for KOPLA® KNL1040:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kopla datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.6 % ISO 294-4, 2577
ASTM Data
Ritiro di stampaggio, parallelo 0.005 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Resistenza a trazione 229 MPa ISO 527
Modulo a flessione 10200 MPa ISO 178
Resistenza alla flessione 311 MPa ISO 178
Resistenza all'urto Charpy, +23°C 59 kJ/m² ISO 179/1eU
Resist. urto Charpy con intaglio, +23°C 26 kJ/m² ISO 179/1eA
Durezza Rockwell R 122 - ISO 2039-2
ASTM Data
Modulo a trazione 13900 MPa ASTM D 638
Resistenza alla trazione 200 MPa ASTM D 638
Modulo a flessione 12100 MPa ASTM D 790
Resistenza alla flessione 295 MPa ASTM D 790
Durezza Rockwell R 122 - ASTM D 785
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 222 °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 210 °C ISO 75-1/-2
Reazione al fuoco a spessore h HB class IEC 60695-11-10
ASTM Data
UL 94 combustibilitá HB - UL 94
DTUL a 264 psi 210 °C ASTM D 648
Temperatura di fusione 222 °C ASTM D 3418
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 3.7 - IEC 62631-2-1
Fattore di dissipazione, 1MHz 0.01 E-4 IEC 62631-2-1
Resistività volumica 1E13 Ohm*m IEC 62631-3-1
Rigidità dielettrica 34 kV/mm IEC 60243-1
ASTM Data
Rigidità elettrica, breve periodo di tempo 22 kV/mm ASTM D 149
Fattore di dissipazione dielèttrica, 1 MHz 0.02 - ASTM D 150
Costante dielèttrica, 1 MHz 3.8 - ASTM D 150
Resistenza di volume 1E15 Ohm*cm ASTM D 257
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.5 % Sim. alla ISO 62
Massa volumica 1440 kg/m³ ISO 1183
Assorbimento d’acqua, 24hr 1 % ASTM D 570
Densità 1450 kg/m³ ASTM D 792
Caratteristiche
Caratteristiche speciali
Alto urto o modificato all'urto
Caratteristiche
Resistenza al scorrimento, Long fiber reinforced
Applicazioni
Automotive, Elettrotecnica ed electrici
Disponibilità geografica
Nord America, Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.