Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KUMHO KTR® 101 - SBS - Kumho Petrochemical Co., Ltd.

Material Data Center offers the following functions for KUMHO KTR® 101:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kumho datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Resistant. Negligible, reversible or no changes in mass and dimensions.

Please consider the information about the application of the materials.
Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Indice di fluidità a caldo, MFI 1 g/10min ASTM D 1238
Temperatura 200 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Resistenza alla trazione 30.4 MPa ASTM D 638
Modulo a 300% allungamento 2.5 MPa ASTM D 412
Durezza A Shore 77 - ASTM D 2240
Altre ProprietàValoreUnitáNorma del test
Densità 940 kg/m³ ASTM D 792
Caratteristiche
Forma fisica disponibile
Pellet
Caratteristiche
Copolimero
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.