Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kurarity™ LA2270 - TPE - Kuraray Co., Ltd.

Material Data Center offers the following functions for Kurarity™ LA2270:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kurarity datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
KURARITY is non-crystalline block copolymer and does not have melting point.
All the KURARITY grades show similar low temperature properties which result from Tg of poly (n-butyl acrylate) or poly (n-butyl acrylate/2-ethylhexyl acrylate) and heat resistance from Tg of PMMA.
LA series : n-butyl acrylate based block copolymers.
Suitable Applications: For Molding, Compound, Additives.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di Fluiditá, MFI 4.8 g/10min ISO 1133
Temperatura 190 °C -
Carico 2.16 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Resist. urto Charpy con intaglio, +23°C N kJ/m² ISO 179/1eA
Resistenza a trazione 15 MPa ISO 37
Durezza Shore A 68 - ISO 7619-1
Durezza Shore D 22 - ISO 7619-1
Other Standards[S]
Carico Unitario al 100% di allungamento 9.3 MPa ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
Proprietà TermicheValoreUnitáNorma del test
Other Standards[S]
Conduttività termica, stato solido 0.15 W/(m K) ASTM E 1530
S: These properties are reported by the producer according standards that are different to our defaults.
Proprietà ElettricheValoreUnitáNorma del test
Other Standards[S]
Fattore di dissipazione dielèttrica, 60 Hz 0.0288 - JIS C 2138
Fattore di dissipazione dielèttrica, 1 MHz 0.0552 - JIS C 2138
Costante dielèttrica, 60 Hz 4.84 - JIS C 2138
Costante dielèttrica, 1 MHz 3.97 - JIS C 2138
S: These properties are reported by the producer according standards that are different to our defaults.
Proprietà OtticheValoreUnitáNorma del test
ISO Data
Opacità 2 - ISO 14782
Other Standards[S]
Trasmissione luminosa 93 % ISO 13468-1
S: These properties are reported by the producer according standards that are different to our defaults.
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1100 kg/m³ ISO 1183
Raccomandazione de Processabilità EstrusioneValoreUnitáNorma del test
Temperatura - Zona di Alimentazione 100 - 130 °C -
Zona 1 140 - 160 °C -
Zona 2 150 - 170 °C -
Temperatura dell ugello 150 - 170 °C -
Caratteristiche
Processabilità e Forma di Forni
Altre Estrusioni
Forma fisica disponibile
Pellet
Caratteristiche speciali
Estab. agli U.V. o per applicaz.in esterni, Trasparente
Caratteristiche
Miscela di resina, Basso odore, Copolimero
Resistenza Chimica
Resistenza all'acido, Resistenza agli alcali, Resistenza all’olio
Applicazioni
Automotive, Elettrotecnica ed electrici
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.