Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kynar Flex® 2900-04 - PVDF - ARKEMA

Material Data Center offers the following functions for Kynar Flex® 2900-04:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kynar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Kynar Flex® resins are fluorinated thermoplastic copolymers.

Kynar Flex® 2900-04 resin is a pelletized, semi-crystalline VF based copolymer. It can be used in extrusion applications such as flexible wire jacketing, or injection molding applications where higher Limiting Oxygen Index is needed for flame and smoke applications.

Additional characteristics:
- Excellent thermal stability
- Excellent abrasion resistance
- Extremely flexible and tough

Meets UL 910 requirements
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 9 cm³/10min ISO 1133
Temperatura 232 °C -
Carico 3.8 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 700 MPa ISO 527
Carico unitario a trazione 25 MPa ISO 527
Deformazione a snervamento 14.5 % ISO 527
Deformazione nominale a rottura >50 % ISO 527
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 143 °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min -40 °C ISO 11357-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 class IEC 60695-11-10
Spessore provato 1.5 mm -
Yellow Card disponibile - -
Reazione al fuoco a spessore h V-0 class IEC 60695-11-10
Spessore provato 0.8 mm -
Indice di ossigeno 75 % ISO 4589-1/-2
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Resistività volumica 2E12 Ohm*m IEC 62631-3-1
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.03 % Sim. alla ISO 62
Massa volumica 1780 kg/m³ ISO 1183
Caratteristiche
Caratteristiche
Copolimero
Disponibilità geografica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.