Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LIM® 6030 - VMQ - Momentive Performance Materials Inc.

Material Data Center offers the following functions for LIM® 6030:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other LIM datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Appearance/Color:
liquid, transparent

Characteristics:
fast cure, high tear strength

Conformity:
The product meets the requirements for passing the test standards USP Class VI, FDA 21 CFR 177.2600 and ISO 10993.
Based on listing of ingredients in the BfR recommendation XV "Silicones", the product is compositionally compliant.

These values were determined with the following conditions:
Postbaked 1 hr @ 204ºC / 400ºF.

Other values were achieved with the following conditions:
As Molded 30 sec @ 177ºC / 350ºF:


Property Value Unit Standard
Shore A hardness, 3s 30 - ISO 868
Tensile Strength 8.3 MPa
ISO 37
Strain at break 750 %
ISO 37
Tear Strength 28.1 kN/m
ASTM D 624
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Resistenza a trazione 9 MPa ISO 37
Deformazione a rottura 675 % ISO 37
Durezza Shore A 35 - ISO 7619-1
ASTM Data
Resistenza alla lacerazione 31 kN/m ASTM D 624
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Yellow Card disponibile - -
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1120 kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Caratteristiche speciali
Trasparente
Certifications
Contatto con gli alimenti, Approvazione per contatto con gli alimenti BfR, Approvato per l'utilizzo per contatto con alimenti secondo la FDA 21 CFR, Approvazione della USP class VI
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.