Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LIGHTER™ S98 - PET - Equipolymers Global

Material Data Center offers the following functions for LIGHTER™ S98:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lighter datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
For more detailed information, please read our brochure p. 46 to 54
or contact our representatives in your region.
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2300 MPa ISO 527
Carico unitario a trazione 55 MPa ISO 527
Deformazione a snervamento 4 % ISO 527
Carico unitario a rottura 24 MPa ISO 527
Deformazione a rottura 250 % ISO 527
Modulo a flessione, 23°C 2100 MPa ISO 178
Resistenza all'urto Izod con intaglio, +23°C 4.5 kJ/m² ISO 180/1A
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 247 °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 78 °C ISO 11357-1/-2
Temp.di rammollimento Vicat, B 77 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 83 E-6/K ISO 11359-1/-2
Altre ProprietàValoreUnitáNorma del test
Viscosità intrinseca 0.84 dl/g -
Acetaldeide 1 ppm -
Color b 2 - CIE
Crystallinity 50 % -
Moisture Content 0.4 % -
Bulk density 880 kg/m³ -
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Temperatura di fusione 277 °C -
Temperatura dello stampo 20 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Soffiaggio
Caratteristiche
Copolimero
Certifications
Contatto con gli alimenti
Applicazioni
Imballaggio
Disponibilità geografica
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.