Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NIPLENE F25 AGR HF - PP-GF25 - Soredi S.p.a.

Material Data Center offers the following functions for NIPLENE F25 AGR HF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Niplene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Indice di fluidità a caldo, MFI 10 g/10min ASTM D 1238
Temperatura 230 °C -
Carico 2.16 kg -
Ritiro di stampaggio, parallelo 0.004 mm/mm ASTM D 955
Ritiro di stampaggio, perpend. 0.006 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Resistenza alla trazione a rottura 85 MPa ASTM D 638
Modulo a flessione 5100 MPa ASTM D 790
Resistenza alla flessione 125 MPa ASTM D 790
Durezza Rockwell R 113 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 115 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 76.9 J/m ASTM D 256
Temperatura -20 °C -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Coeff.di dilatazione termica lin. , perpend. 30 E-6/K ISO 11359-1/-2
ASTM Data
UL 94 combustibilitá HB - UL 94
Spessore testati 1.6 mm -
DTUL a 264 psi 152 °C ASTM D 648
Temp.di rammollimento Vicat 140 °C ASTM D 1525
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 2.7 - IEC 62631-2-1
Resistività volumica 1E13 Ohm*m IEC 62631-3-1
Resistività superficiale 1E14 Ohm IEC 62631-3-2
Rigidità dielettrica 60 kV/mm IEC 60243-1
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'umidità 0.2 % Sim. alla ISO 62
Densità 1080 kg/m³ ASTM D 792
Caratteristiche
Caratteristiche
Rafforzamento accoppiato chimicamente, Omopolimero
Disponibilità geografica
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.