Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Nypel® 6235G UN - PA6-GF35 - BASF

Material Data Center offers the following functions for Nypel® 6235G UN:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Nypel datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Nypel 6235G UN is a 35% glass reinforced injection molding grade of PA6. Based on recycled polyamide feedstocks, Nypel 6235G UN offers a balance of mechanical properties with the ability to pigment with a full range of colorants.

Nypel 6235G UN is recommended for lawn and power equipment housings, structural furniture components such as seat frames, and automotive and industrial applications.
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 10655 / 7205 MPa ISO 527
Carico unitario a rottura 169 / 116 MPa ISO 527
Deformazione a rottura 3.6 / 7.6 % ISO 527
Resistenza all'urto Charpy, +23°C 96 / 110 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 93 / 92 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 18 / 23 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 15 / 14 kJ/m² ISO 179/1eA
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 207 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 217 / * °C ISO 75-1/-2
Altre Proprietàsecco/condUnitáNorma del test
Massa volumica 1360 / - kg/m³ ISO 1183
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 °C -
Pre-essiccamento - Tempo 4 h -
Temperatura di fusione 270 - 290 °C -
Temperatura dello stampo 80 - 90 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Certifications
Contenuto di resina riciclata
Applicazioni
Automotive
Disponibilità geografica
Nord America
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 270 - 290 °C
injection molding, Melt temperature, recommended: 280 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.