Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Panlite® LV-2250Z - PC - Teijin Chemicals Ltd.

Material Data Center offers the following functions for Panlite® LV-2250Z:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Panlite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 8 cm³/10min ISO 1133
Temperatura 300 °C -
Carico 1.2 kg -
ASTM Data
Ritiro di stampaggio, parallelo 0.006 mm/mm ASTM D 955
Ritiro di stampaggio, perpend. 0.006 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2400 MPa ISO 527
Carico unitario a trazione 61 MPa ISO 527
Deformazione a snervamento 6 % ISO 527
Deformazione nominale a rottura >50 % ISO 527
Modulo a flessione, 23°C 2350 MPa ISO 178
Resistenza alla flessione 93 MPa ISO 178
Resistenza all'urto Charpy, +23°C N kJ/m² ISO 179/1eU
Resist. urto Charpy con intaglio, +23°C 76 kJ/m² ISO 179/1eA
ASTM Data
Modulo a trazione 2120 MPa ASTM D 638
Resistenza alla trazione di snervamento 62 MPa ASTM D 638
Resistenza alla trazione a rottura 80 MPa ASTM D 638
Allungamento a snervamento 6 % ASTM D 638
Allungamento a rottura 140 % ASTM D 638
Resistenza a compressione 76 MPa ASTM D 695
Modulo a flessione 2230 MPa ASTM D 790
Resistenza alla flessione 92 MPa ASTM D 790
Durezza Rockwell M 77 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 880 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, 1/4 in 140 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 129 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 142 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 149 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 70 E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin. , perpend. 70 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-2 class IEC 60695-11-10
Spessore provato 1.5 mm -
Reazione al fuoco a spessore h V-2 class IEC 60695-11-10
Spessore provato 0.4 mm -
Glow Wire Flammability Index (GWFI) 825 °C IEC 60695-2-12
GWFI - thickness tested (1) 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 3 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (1) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (2) 3 mm -
ASTM Data
UL 94 combustibilitá V-2 - UL 94
Spessore testati 3 mm -
coefficiente d’espansione termica, lung. 70 E-6/K ASTM D 696
Coefficiente d’espansione termica, tras. 70 E-6/K ASTM D 696
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3.1 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 10 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 90 E-4 IEC 62631-2-1
Resistività volumica >1E13 Ohm*m IEC 62631-3-1
Resistività superficiale >1E15 Ohm IEC 62631-3-2
Rigidità dielettrica 30 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 225 - IEC 60112
ASTM Data
Rigidità elettrica, breve periodo di tempo 30 kV/mm ASTM D 149
Fattore di dissipazione dielèttrica, 60 Hz 0.0004 - ASTM D 150
Fattore di dissipazione dielèttrica, 1 MHz 0.009 - ASTM D 150
Costante dielèttrica, 60 Hz 2.95 - ASTM D 150
Costante dielèttrica, 1 MHz 2.9 - ASTM D 150
Resistenza di volume 3E16 Ohm*cm ASTM D 257
Resistenza all’arco 100 s ASTM D 495
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Trasmissione luminosa 88 % ASTM D 1003
Indice di rifrazione 1.58 - ASTM D 542
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1200 kg/m³ ISO 1183
Assorbimento d’acqua, equilibrio 0.2 % ASTM D 570
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 120 °C -
Pre-essiccamento - Tempo >5 h -
Temperatura di fusione 270 - 320 °C -
Temperatura dello stampo 80 - 120 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Additivi
Agente di distacco
Caratteristiche speciali
Estab. agli U.V. o per applicaz.in esterni, Trasparente
Applicazioni
Polivalente
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.