Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® 7033 SP 01 - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® 7033 SP 01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Polyether block amide Pebax® 7033 SP 01 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
This SP grade has been developed to be heat and UV resistant.


Main applications:
  • Athletic foot wear components
  • Ski shoes
  • Tennis racket bumpers
  • Zip fasteners


Packaging:

This grade is delivered dried in sealed packaging (20 or 25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 414 / 384 MPa ISO 527
Carico unitario a trazione 23 / 22 MPa ISO 527
Deformazione a snervamento 22 / 20 % ISO 527
Deformazione nominale a rottura >50 / >50 % ISO 527
Resistenzia all'urto Charpy con intaglio, +23°C - / 120 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C - / 20 kJ/m² ISO 179/1eA
Carico Unitario al 10% di allungamento 22 / * MPa ISO 527
Carico Unitario al 100% di allungamento 21 / * MPa ISO 527
Carico Unitario a rottura TPE 54 / * MPa ISO 527
Allungamento a rottura TPE >300 / * % ISO 527
Resistenza alla lacerazione 149 / * kN/m ISO 34-1
Durezza Shore D 61 / * - ISO 7619-1
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 172 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 0.45 MPa 99 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 106 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 160 / * E-6/K ISO 11359-1/-2
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Resistività superficiale * / 4E13 Ohm IEC 62631-3-2
Res. Alle correnti striscianti superficiali * / 600 - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 1.1 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.7 / * % Sim. alla ISO 62
Massa volumica 1010 / - kg/m³ ISO 1183
Funzioni
Viscosità-Velocità di taglio , Pebax® 7033 SP 01, TPA, ARKEMA
Sforzo di taglio-Velocità di taglio , Pebax® 7033 SP 01, TPA, ARKEMA
Modulo dinamico a taglio-temperatura , Pebax® 7033 SP 01 (Secco), TPA, ARKEMA
Sforzi-deformazione , Pebax® 7033 SP 01 (Secco), TPA, ARKEMA
Modulo secante-deformazione , Pebax® 7033 SP 01 (Secco), TPA, ARKEMA
Sforzi-deformazioni (isocrona) 23°C, Pebax® 7033 SP 01 (Secco), TPA, ARKEMA
Modulo di scorrimento-tempo 23°C, Pebax® 7033 SP 01 (Secco), TPA, ARKEMA
Curva di scorrimento 23°C, Pebax® 7033 SP 01 (Secco), TPA, ARKEMA
Sforzi-deformazioni (isocrona) 40°C, Pebax® 7033 SP 01 (Secco), TPA, ARKEMA
Modulo di scorrimento-tempo 40°C, Pebax® 7033 SP 01 (Secco), TPA, ARKEMA
Curva di scorrimento 40°C, Pebax® 7033 SP 01 (Secco), TPA, ARKEMA
Sforzi-deformazioni (isocrona) 80°C, Pebax® 7033 SP 01 (Secco), TPA, ARKEMA
Modulo di scorrimento-tempo 80°C, Pebax® 7033 SP 01 (Secco), TPA, ARKEMA
Curva di scorrimento 80°C, Pebax® 7033 SP 01 (Secco), TPA, ARKEMA
Volume specifico-temperatura (pvT) , Pebax® 7033 SP 01, TPA, ARKEMA
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione Film, Estrusione Profilati, Altre Estrusioni, Stampaggio a Trasferimento, Colata, Termoformatura
Forma fisica disponibile
Pellet
Caratteristiche speciali
Galvanizzabile, Stabilizzato o stabile alla luce, Estab. agli U.V. o per applicaz.in esterni, Stabilizzato o stabile al calore
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 230°C / 260°C / 290°C
- Typical mold temperature : 25 – 60°C
- Drying time and temperature (only necessary for bags opened for more than two hours) : 5-7 hours at 70-80°C
Altre Estrusioni

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 220°C / 235°C / 250°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 5-7 hours at 70-80°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.