Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® B 409 Pellets - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® B 409 Pellets:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Platamid® B 409 Pellets
Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® B 409 is a high molecular weight, high melting temperature range, partially crystalline copolyamide delivered in pellet form. The special interest of this product is the combination of high melting temperature and high melt viscosity.

Platamid® B 409 can be applied out of a cresolic solution. The thermal activation of the hot melt layer can be accomplished by means of induction of hot air.



AVAILABLE GRADES
This grade is available:
- dried with lubricant (B 409 TL)
- undried with lubricant (B 409 FL)
PACKAGING
Platamid® B 409 TL is delivered in 25 kg sealed bags.
Platamid® B 409 FL is delivered in 25 kg sealed bags.
These grades are ready to be processed.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 7.2 / * cm³/10min ISO 1133
Temperatura 200 / * °C -
Carico 2.16 / * kg -
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 178 / * °C ISO 11357-1/-3
Altre Proprietàsecco/condUnitáNorma del test
Massa volumica 1100 / - kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Estrusione Film
Forma fisica disponibile
Pellet
Additivi
Lubrificanti
Caratteristiche
Copolimero
Disponibilità geografica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.