Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® BESNO TL - PA11 - ARKEMA

Material Data Center offers the following functions for Rilsan® BESNO TL:
unit conversion, PDF datasheet print, parameters for material models, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
PA11,EHL,22-010
Rilsan® BESNO TL resin is a polyamide 11 produced from a renewable source. This natural grade is designed for extrusion.



Main applications:
  • Fluid transportation


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags, 44 lb bags, 1000 lb rigid containers) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 1 / * cm³/10min ISO 1133
Temperatura 235 / * °C -
Carico 2.16 / * kg -
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione - / 1280 MPa ISO 527
Carico unitario a trazione - / 38 MPa ISO 527
Deformazione a snervamento - / 5 % ISO 527
Deformazione nominale a rottura - / >50 % ISO 527
Resistenzia all'urto Charpy con intaglio, +23°C - / 11 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C - / 12 kJ/m² ISO 179/1eA
Perforazione-forza massima, -30°C - / 6000 N ISO 6603-2
Energia di perforazione, -30°C - / 70 J ISO 6603-2
Durezza Shore D 72 / * - ISO 7619-1
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 186 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 50 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 145 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 160 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 85 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Yellow Card disponibile sì / * - -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3 / - - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3 / - - IEC 62631-2-1
Fattore di dissipazione, 100Hz 308 / - E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 183 / - E-4 IEC 62631-2-1
Resistività volumica - / 1E12 Ohm*m IEC 62631-3-1
Resistività superficiale * / 1E14 Ohm IEC 62631-3-2
Rigidità dielettrica - / 30 kV/mm IEC 60243-1
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 1.9 / * % Sim. alla ISO 62
Massa volumica 1020 / 1020 kg/m³ ISO 1183
Biobased content 96 % -
Funzioni
Viscosità-Velocità di taglio , Rilsan® BESNO TL, PA11, ARKEMA
Sforzo di taglio-Velocità di taglio , Rilsan® BESNO TL, PA11, ARKEMA
Modulo dinamico a taglio-temperatura , Rilsan® BESNO TL (Secco), PA11, ARKEMA
Sforzi-deformazione , Rilsan® BESNO TL (Secco), PA11, ARKEMA
Modulo secante-deformazione , Rilsan® BESNO TL (Secco), PA11, ARKEMA
Sforzi-deformazioni (isocrona) 23°C, Rilsan® BESNO TL (Secco), PA11, ARKEMA
Modulo di scorrimento-tempo 23°C, Rilsan® BESNO TL (Secco), PA11, ARKEMA
Curva di scorrimento 23°C, Rilsan® BESNO TL (Secco), PA11, ARKEMA
Sforzi-deformazioni (isocrona) 80°C, Rilsan® BESNO TL (Secco), PA11, ARKEMA
Modulo di scorrimento-tempo 80°C, Rilsan® BESNO TL (Secco), PA11, ARKEMA
Curva di scorrimento 80°C, Rilsan® BESNO TL (Secco), PA11, ARKEMA
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione Film, Estrusione Profilati, Estrusione di Lastre/Fogli, Altre Estrusioni
Forma fisica disponibile
Pellet
Additivi
Lubrificanti
Caratteristiche speciali
Stabilizzato o stabile alla luce, Estab. agli U.V. o per applicaz.in esterni, Stabilizzato o stabile al calore
Certifications
Contiene risorse rinnovabili
Disponibilità geografica
Altre informazioni
Altre Estrusioni

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 280°C.

- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 80-90°C.
Resistenza chimica
Acidi
Acido acetico (5% da massa) (23°C)
Soluzione acida citrica (10% da massa) (23°C)
Acido lattico (10% da massa) (23°C)
Acido cloridrico (36% da massa) (23°C)
Acido nitrico (40% da massa) (23°C)
Acido solforico (38% da massa) (23°C)
Acido solforico (5% da massa) (23°C)
Soluzione acida cromica (40% da massa) (23°C)
Basi
Soluzione dell' idrossido del sodio (35% da massa) (23°C)
Soluzione dell' idrossido del sodio (1% da massa) (23°C)
Soluzione dell' idrossido di ammonio (10% da massa) (23°C)
Alcool
Metanolo (23°C)
Etanolo (23°C)
Idrocarburi
n-Hexane (23°C)
Toluene (23°C)
Chetoni
Acetone (23°C)
Oli minerali
Olio multigrade del motore di SAE 10W40 (23°C)
Olio multigrade del motore di SAE 10W40 (130°C)
Olio dell' ipoide-ingranaggio di SAE 80/90 (130°C)
Olio isolante (23°C)
Combustibili Standard
Liquido 1 di ISO 1817 (60°C)
Liquido 2 di ISO 1817 (60°C)
Liquido 3 di ISO 1817 (60°C)
Liquido 4 di ISO 1817 (60°C)
Combust. stand. senza alcool (pref. ISO 1817 liquido C) (23°C)
Combust. stand. con alcool (pref. ISO 1817 liquido 4) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (90°C)
Combustibile diesel (pref. ISO 1817 liquido F) (>90°C)
Soluzioni saline
Soluzione del cloruro di sodio (10% da massa) (23°C)
Soluzione dell' ipoclorito del sodio (10% da massa) (23°C)
Soluzione del cloruro dello zinco (50% da massa) (23°C)
Altri
Acetato etilico (23°C)
Perossido di idrogeno (23°C)
Liquido di freno del DOT N° 4 (130°C)
Glicol etilenico (50% da massa) in acqua (108°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.