Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® BMNO P20 TLD - PA11 - ARKEMA

Material Data Center offers the following functions for Rilsan® BMNO P20 TLD:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
PA11-P, MHLR, 12-005
Rilsan® BMNO P20 TLD resin is a polyamide 11 produced from a renewable source. This natural grade is plasticized and designed for injection molding.



Main applications:
  • Tennis racquet bumpers

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 32 / * cm³/10min ISO 1133
Temperatura 235 / * °C -
Carico 2.16 / * kg -
Ritiro di stampaggio, parallelo 1.3 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.4 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione - / 545 MPa ISO 527
Carico unitario a trazione - / 32 MPa ISO 527
Deformazione a snervamento - / 30 % ISO 527
Deformazione nominale a rottura - / >50 % ISO 527
Resistenzia all'urto Charpy con intaglio, -30°C - / 7 kJ/m² ISO 179/1eA
Durezza Shore D 61 / * - ISO 7619-1
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 186 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 47 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 135 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 145 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 100 / * E-6/K ISO 11359-1/-2
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 7 / - - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3 / - - IEC 62631-2-1
Fattore di dissipazione, 100Hz 1900 / - E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 614 / - E-4 IEC 62631-2-1
Resistività volumica - / 1E10 Ohm*m IEC 62631-3-1
Resistività superficiale * / 2E12 Ohm IEC 62631-3-2
Rigidità dielettrica - / 26 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali * / 600 - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 1.8 / * % Sim. alla ISO 62
Massa volumica 1050 / 1050 kg/m³ ISO 1183
Biobased content 92 % -
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 - 90 °C -
Pre-essiccamento - Tempo 4 - 6 h -
Temperatura di fusione 210 - 280 °C -
Temperatura dello stampo 20 - 60 °C -
Funzioni
Viscosità-Velocità di taglio , Rilsan® BMNO P20 TLD, PA11, ARKEMA
Sforzo di taglio-Velocità di taglio , Rilsan® BMNO P20 TLD, PA11, ARKEMA
Modulo dinamico a taglio-temperatura , Rilsan® BMNO P20 TLD (Secco), PA11, ARKEMA
Sforzi-deformazione , Rilsan® BMNO P20 TLD (Secco), PA11, ARKEMA
Modulo secante-deformazione , Rilsan® BMNO P20 TLD (Secco), PA11, ARKEMA
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Additivi
Agente di distacco, Plastificante
Caratteristiche speciali
Stabilizzato o stabile alla luce, Estab. agli U.V. o per applicaz.in esterni, Stabilizzato o stabile al calore
Certifications
Contiene risorse rinnovabili
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 210°C / 230°C / 280°C.
- Mold temperature : 20 - 60°C

- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80-90°C.
Resistenza chimica
Acidi
Acido acetico (5% da massa) (23°C)
Soluzione acida citrica (10% da massa) (23°C)
Acido lattico (10% da massa) (23°C)
Acido cloridrico (36% da massa) (23°C)
Acido nitrico (40% da massa) (23°C)
Acido solforico (38% da massa) (23°C)
Acido solforico (5% da massa) (23°C)
Soluzione acida cromica (40% da massa) (23°C)
Basi
Soluzione dell' idrossido del sodio (35% da massa) (23°C)
Soluzione dell' idrossido del sodio (1% da massa) (23°C)
Soluzione dell' idrossido di ammonio (10% da massa) (23°C)
Alcool
Metanolo (23°C)
Etanolo (23°C)
Idrocarburi
n-Hexane (23°C)
Toluene (23°C)
Chetoni
Acetone (23°C)
Oli minerali
Olio multigrade del motore di SAE 10W40 (23°C)
Olio multigrade del motore di SAE 10W40 (130°C)
Olio dell' ipoide-ingranaggio di SAE 80/90 (130°C)
Olio isolante (23°C)
Combustibili Standard
Liquido 1 di ISO 1817 (60°C)
Liquido 2 di ISO 1817 (60°C)
Liquido 3 di ISO 1817 (60°C)
Liquido 4 di ISO 1817 (60°C)
Combust. stand. senza alcool (pref. ISO 1817 liquido C) (23°C)
Combust. stand. con alcool (pref. ISO 1817 liquido 4) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (90°C)
Combustibile diesel (pref. ISO 1817 liquido F) (>90°C)
Soluzioni saline
Soluzione del cloruro di sodio (10% da massa) (23°C)
Soluzione dell' ipoclorito del sodio (10% da massa) (23°C)
Soluzione del cloruro dello zinco (50% da massa) (23°C)
Altri
Acetato etilico (23°C)
Perossido di idrogeno (23°C)
Liquido di freno del DOT N° 4 (130°C)
Glicol etilenico (50% da massa) in acqua (108°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.