Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TENAC™-C MT754 - POM-MF20 - Asahi Kasei

Material Data Center offers the following functions for TENAC™-C MT754:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tenac datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 15 cm³/10min ISO 1133
Temperatura 190 °C -
Carico 2.16 kg -
Indice di Fluiditá, MFI 20 g/10min ISO 1133
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 4800 MPa ISO 527
Carico unitario a rottura 61 MPa ISO 527
Deformazione a rottura 5 % ISO 527
Modulo a flessione, 23°C 4800 MPa ISO 178
Resistenzia all'urto Charpy con intaglio, +23°C 3 kJ/m² ISO 179/1eA
ASTM Data
Resistenza alla trazione 60 MPa ASTM D 638
Allungamento a rottura 7 % ASTM D 638
Modulo a flessione 5000 MPa ASTM D 790
Resistenza alla flessione 108 MPa ASTM D 790
Durezza Rockwell M 98 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 39 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 131 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 161 °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 60 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.5 mm -
Yellow Card disponibile - -
Reazione al fuoco a spessore h HB class IEC 60695-11-10
Spessore provato 0.8 mm -
Yellow Card disponibile - -
ASTM Data
UL 94 combustibilitá HB - UL 94
coefficiente d’espansione termica, lung. 60 E-6/K ASTM D 696
DTUL a 66 psi 163 °C ASTM D 648
DTUL a 264 psi 150 °C ASTM D 648
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1580 kg/m³ ISO 1183
Assorbimento d’acqua, 24hr 0.2 % ASTM D 570
Densità 1580 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 - 90 °C -
Pre-essiccamento - Tempo 3 - 4 h -
Temperatura di fusione 180 - 210 °C -
Temperatura dello stampo 60 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Altre Estrusioni
Forma fisica disponibile
Pellet
Caratteristiche
Bassa deformazione, Copolimero
Applicazioni
Automotive
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.