Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TROGAMID® CX9710 NC - PAPACM12 - Evonik Operations GmbH

Material Data Center offers the following functions for TROGAMID® CX9710 NC:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Trogamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

Medium-viscosity and transparent polyamide for injection molding with release agent

TROGAMID® CX9710 is a medium-viscosity and transparent polyamide for injection molding for the manufacture of parts in the optical industry.

The material absorbs only small amounts of water. Components made from this material therefore show excellent dimensional stability under changing ambient humidity as well as consistent UV-stability and chemical resistance. 

TROGAMID® CX9710 is supplied as spherical pellets in moisture-proof packaging.

Pigmentation may affect values.

For information about processing of TROGAMID®, please follow the general recommendations about “Processing of TROGAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

 


FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.TROGAMID.COM
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 20 / * cm³/10min ISO 1133
Temperatura 285 / * °C -
Carico 5 / * kg -
Ritiro di stampaggio, parallelo 0.7 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.8 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 1400 / - MPa ISO 527
Carico unitario a trazione 60 / - MPa ISO 527
Deformazione a snervamento 8 / - % ISO 527
Deformazione nominale a rottura >50 / - % ISO 527
Modulo di scorrimento a trazione, 1h * / 1400 MPa ISO 899-1
Modulo di scorrimento a trazione, 1000h * / 700 MPa ISO 899-1
Resistenza all'urto Charpy, +23°C N / - kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C N / - kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 11 / 10.5 kJ/m² ISO 179/1eA
Type of failure C / C - -
Resistenzia all'urto Charpy con intaglio, -30°C 13 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Durezza Shore D 81 / * - ISO 7619-1
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 250 / * °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 140 / * °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 108 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 122 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 130 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 90 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 90 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Reazione al fuoco a spessore h HB / * class IEC 60695-11-10
Spessore provato 0.8 / * mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3.6 / - - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3.2 / - - IEC 62631-2-1
Fattore di dissipazione, 100Hz 120 / - E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 325 / - E-4 IEC 62631-2-1
Resistività superficiale * / 1E13 Ohm IEC 62631-3-2
Res. Alle correnti striscianti superficiali 600 / - - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 3.5 / * % Sim. alla ISO 62
Assorbimento d'umidità 1.5 / * % Sim. alla ISO 62
Massa volumica 1020 / - kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 280 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 80 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Stamp. ad Iniezione, pressione di chiusura 70 MPa ISO 294
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione Film, Estrusione Profilati, Estrusione di Lastre/Fogli, Altre Estrusioni, Soffiaggio, Termoformatura
Forma fisica disponibile
Pellet, Colore naturale
Additivi
Agente di distacco
Caratteristiche speciali
Stabilizzato o stabile alla luce, Estab. agli U.V. o per applicaz.in esterni, Trasparente
Resistenza Chimica
Resistenza chimica generale
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.