Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 4520 FC R01 - PBT - BASF

Material Data Center offers the following functions for Ultradur® B 4520 FC R01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Ultradur® B4520 FC R01 UN is suitable for plastic parts, where material approval direct food contact is a mandatory requirement.

The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulations including European Food Contact (EU) Nr. 10/2011 and GMP (EC) N°2023/2006.

For questions regarding the compliance with further regulations, and certificates, please contact your local BASF representative or Plastics Safety (E-Mail: plastics.safety@basf.com).

The products can also be offered as BMBcert™ and/or Ccycled™. Due to the Massbalance approach the product properties do not change.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 24 cm³/10min ISO 1133
Temperatura 250 °C -
Carico 2.16 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2500 MPa ISO 527
Carico unitario a trazione 56 MPa ISO 527
Deformazione a snervamento 3.6 % ISO 527
Deformazione nominale a rottura >50 % ISO 527
Resistenza all'urto Charpy, +23°C 260 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 200 kJ/m² ISO 179/1eU
Type of failure C - -
Resistenzia all'urto Charpy con intaglio, +23°C 3.5 kJ/m² ISO 179/1eA
Type of failure C - -
Resistenzia all'urto Charpy con intaglio, -30°C 3 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 223 °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 0.45 MPa 130 °C ISO 75-1/-2
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1300 kg/m³ ISO 1183
Proprietà Specifiche MaterialeValoreUnitáNorma del test
ISO Data
Numero di viscosità 120 cm³/g ISO 307, 1157, 1628
Caratteristiche
Certifications
Contatto con gli alimenti, Approvato per l'utilizzo per contatto con alimenti 10/2011, Approvato per l'utilizzo per contatto con alimenti secondo la FDA 21 CFR
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 275 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 70 °C
injection molding, Mold temperature, recommended: 60 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com