Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultraform® W2320 003 BK Q600 - POM - BASF

Material Data Center offers the following functions for Ultraform® W2320 003 BK Q600:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Very free-flowing, rapidly solidifying grade for use where processing is extremely difficult but mechanical properties are lower.

Abbreviated designation according to ISO 1043-1: POM
Designation according to ISO 29988-POM-K,,M-GCR,5-2
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 25 cm³/10min ISO 1133
Temperatura 190 °C -
Carico 2.16 kg -
Ritiro di stampaggio, parallelo 1.9 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.8 % ISO 294-4, 2577
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2700 MPa ISO 527
Carico unitario a trazione 63 MPa ISO 527
Deformazione a snervamento 8.5 % ISO 527
Deformazione nominale a rottura 25 % ISO 527
Modulo di scorrimento a trazione, 1h 2000 MPa ISO 899-1
Modulo di scorrimento a trazione, 1000h 1350 MPa ISO 899-1
Resistenzia all'urto Charpy con intaglio, +23°C 4.5 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 167 °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 95 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 156 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 150 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 110 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.6 mm -
Yellow Card disponibile - -
Reazione al fuoco a spessore h HB class IEC 60695-11-10
Spessore provato 0.8 mm -
Yellow Card disponibile - -
Indice di ossigeno 15 % ISO 4589-1/-2
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3.8 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3.8 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 10 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 65 E-4 IEC 62631-2-1
Resistività volumica 1E12 Ohm*m IEC 62631-3-1
Resistività superficiale 1E15 Ohm IEC 62631-3-2
Rigidità dielettrica 40 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 600 - IEC 60112
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.8 % Sim. alla ISO 62
Assorbimento d'umidità 0.2 % Sim. alla ISO 62
Massa volumica 1410 kg/m³ ISO 1183
Funzioni
Viscosità-Velocità di taglio , Ultraform® W2320 003 BK Q600, POM, BASF
Sforzo di taglio-Velocità di taglio , Ultraform® W2320 003 BK Q600, POM, BASF
Modulo dinamico a taglio-temperatura , Ultraform® W2320 003 BK Q600, POM, BASF
Sforzi-deformazione , Ultraform® W2320 003 BK Q600, POM, BASF
Modulo secante-deformazione , Ultraform® W2320 003 BK Q600, POM, BASF
Sforzi-deformazioni (isocrona) 23°C, Ultraform® W2320 003 BK Q600, POM, BASF
Modulo di scorrimento-tempo 23°C, Ultraform® W2320 003 BK Q600, POM, BASF
Curva di scorrimento 23°C, Ultraform® W2320 003 BK Q600, POM, BASF
Sforzi-deformazioni (isocrona) 40°C, Ultraform® W2320 003 BK Q600, POM, BASF
Modulo di scorrimento-tempo 40°C, Ultraform® W2320 003 BK Q600, POM, BASF
Curva di scorrimento 40°C, Ultraform® W2320 003 BK Q600, POM, BASF
Sforzi-deformazioni (isocrona) 60°C, Ultraform® W2320 003 BK Q600, POM, BASF
Modulo di scorrimento-tempo 60°C, Ultraform® W2320 003 BK Q600, POM, BASF
Curva di scorrimento 60°C, Ultraform® W2320 003 BK Q600, POM, BASF
Sforzi-deformazioni (isocrona) 80°C, Ultraform® W2320 003 BK Q600, POM, BASF
Modulo di scorrimento-tempo 80°C, Ultraform® W2320 003 BK Q600, POM, BASF
Curva di scorrimento 80°C, Ultraform® W2320 003 BK Q600, POM, BASF
Sforzi-deformazioni (isocrona) 100°C, Ultraform® W2320 003 BK Q600, POM, BASF
Modulo di scorrimento-tempo 100°C, Ultraform® W2320 003 BK Q600, POM, BASF
Curva di scorrimento 100°C, Ultraform® W2320 003 BK Q600, POM, BASF
Sforzi-deformazioni (isocrona) 120°C, Ultraform® W2320 003 BK Q600, POM, BASF
Modulo di scorrimento-tempo 120°C, Ultraform® W2320 003 BK Q600, POM, BASF
Curva di scorrimento 120°C, Ultraform® W2320 003 BK Q600, POM, BASF
Volume specifico-temperatura (pvT) , Ultraform® W2320 003 BK Q600, POM, BASF
Modulo a taglio-temperatura , Ultraform® W2320 003 BK Q600, POM, BASF
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet, Nero
Additivi
Agente di distacco
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
injection molding, Melt temperature, range: 185 - 230 °C
injection molding, Melt temperature, recommended: 200 °C
injection molding, Mold temperature, range: 60 - 100 °C
injection molding, Mold temperature, recommended: 90 °C
injection molding, Dwell time, thermoplastics: 10 min
Resistenza chimica
Acidi
Acido acetico (5% da massa) (23°C)
Acido lattico (10% da massa) (23°C)
Acido cloridrico (36% da massa) (23°C)
Acido nitrico (40% da massa) (23°C)
Acido solforico (38% da massa) (23°C)
Acido solforico (5% da massa) (23°C)
Soluzione acida cromica (40% da massa) (23°C)
Basi
Soluzione dell' idrossido del sodio (35% da massa) (23°C)
Soluzione dell' idrossido del sodio (1% da massa) (23°C)
Soluzione dell' idrossido di ammonio (10% da massa) (23°C)
Alcool
Alcool di isopropile (23°C)
Metanolo (23°C)
Etanolo (23°C)
Idrocarburi
n-Hexane (23°C)
Toluene (23°C)
isoottano (23°C)
Chetoni
Acetone (23°C)
Eteri
Etere Etilico (23°C)
Oli minerali
Olio multigrade del motore di SAE 10W40 (130°C)
Olio dell' ipoide-ingranaggio di SAE 80/90 (130°C)
Combustibili Standard
Liquido 1 di ISO 1817 (60°C)
Liquido 2 di ISO 1817 (60°C)
Liquido 3 di ISO 1817 (60°C)
Liquido 4 di ISO 1817 (60°C)
Combust. stand. senza alcool (pref. ISO 1817 liquido C) (23°C)
Combust. stand. con alcool (pref. ISO 1817 liquido 4) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (>90°C)
Soluzioni saline
Soluzione del cloruro di sodio (10% da massa) (23°C)
Soluzione dell' ipoclorito del sodio (10% da massa) (23°C)
Soluzione del carbonato di sodio (20% da massa) (23°C)
Soluzione del carbonato di sodio (2% da massa) (23°C)
Altri
Acetato etilico (23°C)
Perossido di idrogeno (23°C)
Liquido di freno del DOT N° 4 (130°C)
Glicol etilenico (50% da massa) in acqua (108°C)
acido oleico 50% + olio di oliva 50% (23°C)
Acqua (23°C)
Acqua deionizzata (90°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.