Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® Advanced T1000HG7 LS BK23593 - PA6T/6I-GF35 - BASF

Material Data Center offers the following functions for Ultramid® Advanced T1000HG7 LS BK23593:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Heat stabilized, partially aromatic polyphthalamide for injection molding with strong mechanical properties especially at elevated temperatures and excellent chemical resistance for highly stressed parts. The product can be characterized as compound with high strength and stiffness, very low water absorption and outstanding dimensional stability. It features a high melting point (320°C) and excellent melt stability.

Markets & applications
Automotive: Fuel system, cooling system, powertrain, thermostat housing, pumps, fuel cell
E&E: Sensors, SMT applications (surface mount technology)
Industry goods: Pumps, compressors
Consumer goods: home appliances, consumer electronics, furniture fittings
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.4 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.9 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 14000 / 14000 MPa ISO 527
Carico unitario a rottura 220 / 210 MPa ISO 527
Deformazione a rottura 2 / 1.9 % ISO 527
Resistenza all'urto Charpy, +23°C 70 / - kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 70 / - kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 8 / - kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 8 / - kJ/m² ISO 179/1eA
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 320 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 280 / * °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 22 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 52 / * E-6/K ISO 11359-1/-2
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Resistività volumica >1E13 / >1E13 Ohm*m IEC 62631-3-1
Resistività superficiale * / >1E15 Ohm IEC 62631-3-2
Rigidità dielettrica 37 / - kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali - / 600 - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 3.8 / * % Sim. alla ISO 62
Assorbimento d'umidità 1.6 / * % Sim. alla ISO 62
Massa volumica 1490 / - kg/m³ ISO 1183
Proprietà Specifiche Materialesecco/condUnitáNorma del test
ISO Data
Numero di viscosità 105 / * cm³/g ISO 307, 1157, 1628
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 350 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 150 °C ISO 294
Funzioni
Sforzi-deformazione , Ultramid® Advanced T1000HG7 LS BK23593 (Secco), PA6T/6I-GF35, BASF
Sforzi-deformazione , Ultramid® Advanced T1000HG7 LS BK23593 (cond.), PA6T/6I-GF35, BASF
Modulo secante-deformazione , Ultramid® Advanced T1000HG7 LS BK23593 (Secco), PA6T/6I-GF35, BASF
Modulo secante-deformazione , Ultramid® Advanced T1000HG7 LS BK23593 (cond.), PA6T/6I-GF35, BASF
Modulo a taglio-temperatura , Ultramid® Advanced T1000HG7 LS BK23593 (Secco), PA6T/6I-GF35, BASF
Modulo a taglio-temperatura , Ultramid® Advanced T1000HG7 LS BK23593 (cond.), PA6T/6I-GF35, BASF
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet, Nero
Caratteristiche speciali
Stabilizzato o stabile al calore
Caratteristiche
Resistenza del fuso
Resistenza Chimica
Resistenza chimica generale
Applicazioni
Automotive, Elettrotecnica ed electrici
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING
Pre/Post-processing, max. allowed water content: .05 %
Pre/Post-processing, Pre-drying, Temperature: 120 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 335 - 355 °C
injection molding, Melt temperature, recommended: 350 °C
injection molding, Mold temperature, range: 140 - 170 °C
injection molding, Mold temperature, recommended: 150 °C
injection molding, Dwell time, thermoplastics: 5 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.