Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrasint PP nat 01 - PP - BASF

Material Data Center offers the following functions for Ultrasint PP nat 01:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrasint datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 14 cm³/10min ISO 1133
Temperatura 220 °C -
Carico 2.16 kg -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 140 °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 62 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 102 °C ISO 75-1/-2
Temp.di rammollimento Vicat, A 131 °C ISO 306
Temp.di rammollimento Vicat, B 90 °C ISO 306
Altre ProprietàValoreUnitáNorma del test
Massa volumica 890 kg/m³ ISO 1183
Bulk density 330 kg/m³ -
3D DataValoreUnitáNorma del test
Other Standards[S]
Modulo a trazione, flat 1400 MPa ISO 527
Modulo a trazione, upright 1400 MPa ISO 527
Resistenza a trazione, flat 28 MPa ISO 527
Resistenza a trazione, upright 28 MPa ISO 527
Deformazione a rottura, flat 30 % ISO 527
Deformazione a rottura, upright 10 % ISO 527
Modulo a flessione, flat 1250 MPa ISO 178
Modulo a flessione, upright 1500 MPa ISO 178
Resistenza all'urto Charpy, +23°C, flat 29 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, +23°C, upright 20 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C, flat 3.3 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, +23°C, upright 3.2 kJ/m² ISO 179/1eA
Resistenza all'urto Izod, +23°C, flat 24 kJ/m² ISO 180/1U
Resistenza all'urto Izod, +23°C, upright 16 kJ/m² ISO 180/1U
Resistenza all'urto Izod con intaglio, +23°C, flat 3.5 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio, +23°C, upright 3 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Caratteristiche
Processabilità e Forma di Forni
Additive Manufacturing, Sinterizzazione a laser
Forma fisica disponibile
Polveri, Colore naturale, Bianco
Caratteristiche speciali
Translucent
Applicazioni
Automotive, Elettrotecnica ed electrici, Medicale, Attrezzature sportive
Disponibilità geografica
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com