Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrason® S 2010 G6 UN - PSU-GF30 - BASF

Material Data Center offers the following functions for Ultrason® S 2010 G6 UN:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Ultrason S datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Medium viscosity injection moulding grade with high rigidity and strength, 30 % glass fiber reinforced
Abbreviated designation according to ISO 1043: PSU-GF30
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 35 / * cm³/10min ISO 1133
Temperatura 360 / * °C -
Carico 10 / * kg -
Ritiro di stampaggio, parallelo 0.3 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.5 / * % ISO 294-4, 2577
Temperatura di estrazione 182 °C -
ASTM Data
Ritiro di stampaggio, parallelo 0.003 mm/mm ASTM D 955
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione - / 9000 MPa ISO 527
Carico unitario a rottura - / 130 MPa ISO 527
Deformazione a rottura - / 3 % ISO 527
Modulo di scorrimento a trazione, 1h * / 8600 MPa ISO 899-1
Resistenza all'urto Charpy, +23°C - / 45 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C - / 50 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C - / 9 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C - / 9 kJ/m² ISO 179/1eA
ASTM Data
Resistenza alla trazione a rottura 126 / - MPa ASTM D 638
Allungamento a rottura 1.8 / - % ASTM D 638
Modulo a flessione 10200 / - MPa ASTM D 790
Resistenza all'urto Izod con intaglio, 1/8 in 10 / - J/m ASTM D 256
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di transizione vetrosa, 10°C/min 187 / * °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 184 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 187 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 190 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 20 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-1 / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Yellow Card disponibile sì / * - -
Reazione al fuoco a spessore h V-0 / * class IEC 60695-11-10
Spessore provato 3.0 / * mm -
Yellow Card disponibile sì / * - -
Indice di ossigeno 37.4 / * % ISO 4589-1/-2
ASTM Data
DTUL a 66 psi 186 °C ASTM D 648
DTUL a 264 psi 183 °C ASTM D 648
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz * / 3.7 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz * / 3.7 - IEC 62631-2-1
Fattore di dissipazione, 100Hz * / 10 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz * / 60 E-4 IEC 62631-2-1
Resistività volumica * / >1E13 Ohm*m IEC 62631-3-1
Resistività superficiale * / >1E15 Ohm IEC 62631-3-2
Rigidità dielettrica * / 45 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali * / 125 - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 0.6 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.2 / * % Sim. alla ISO 62
Massa volumica 1460 / - kg/m³ ISO 1183
Densità 1490 kg/m³ ASTM D 792
Proprietà Specifiche Materialesecco/condUnitáNorma del test
ISO Data
Numero di viscosità 63 / * cm³/g ISO 307, 1157, 1628
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 360 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 150 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Stamp. ad Iniezione, pressione di chiusura 80 MPa ISO 294
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 140 °C -
Pre-essiccamento - Tempo 4 h -
Umidità del Processo ≤0.02 % -
Temperatura di fusione 350 - 390 °C -
Temperatura dello stampo 130 - 180 °C -
Funzioni
Viscosità-Velocità di taglio , Ultrason® S 2010 G6 UN, PSU-GF30, BASF
Sforzo di taglio-Velocità di taglio , Ultrason® S 2010 G6 UN, PSU-GF30, BASF
Modulo dinamico a taglio-temperatura , Ultrason® S 2010 G6 UN (Secco), PSU-GF30, BASF
Sforzi-deformazione , Ultrason® S 2010 G6 UN (cond.), PSU-GF30, BASF
Modulo secante-deformazione , Ultrason® S 2010 G6 UN (cond.), PSU-GF30, BASF
Sforzi-deformazioni (isocrona) 23°C, Ultrason® S 2010 G6 UN (cond.), PSU-GF30, BASF
Modulo di scorrimento-tempo 23°C, Ultrason® S 2010 G6 UN (cond.), PSU-GF30, BASF
Curva di scorrimento 23°C, Ultrason® S 2010 G6 UN (cond.), PSU-GF30, BASF
Sforzi-deformazioni (isocrona) 140°C, Ultrason® S 2010 G6 UN (Secco), PSU-GF30, BASF
Modulo di scorrimento-tempo 140°C, Ultrason® S 2010 G6 UN (Secco), PSU-GF30, BASF
Curva di scorrimento 140°C, Ultrason® S 2010 G6 UN (Secco), PSU-GF30, BASF
Volume specifico-temperatura (pvT) , Ultrason® S 2010 G6 UN, PSU-GF30, BASF
Modulo a taglio-temperatura , Ultrason® S 2010 G6 UN (cond.), PSU-GF30, BASF
Fatigue strength , Ultrason® S 2010 G6 UN, PSU-GF30, BASF
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione Profilati, Estrusione di Lastre/Fogli
Forma fisica disponibile
Pellet, Colore naturale
Caratteristiche speciali
Galvanizzabile
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING
Pre/Post-processing, max. allowed water content: .02 %
Pre/Post-processing, Pre-drying, Temperature: 140 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 350 - 390 °C
injection molding, Melt temperature, recommended: 360 °C
injection molding, Mold temperature, range: 130 - 180 °C
injection molding, Mold temperature, recommended: 150 °C
injection molding, Dwell time, thermoplastics: 10 min

Pretreatment
Drying temperature: 130 - 150°C
Drying time: minimum 4h
recommended dryer: vaccum or dry air dryer
maximum moisture: 0,02 - 0,05%

Ultrason® can be injection molded by any type of machinery on the market, provided that the plasticizing unit and the mold temperature control system have been configured appropriately. The machinery manufacturer must be consulted if any doubts exist on the ability of various parts to withstand the high temperatures required (e.g. barrel, barrel head, bolted connections, etc.)

Long residence time in combination with high temperatures should be avoided e.g. by pump out material at regular intervals.
During extended interruptions, the barrel temperature should be lowered to about 250-280°C.

It has been found out that heating to the requested processing temperature and shutting down or lowering the temperature is best carried out in two steps.
First, the barrel temperatures are set at the lower processing temperature range for the particular thermoplastic (340 - 350 °C). As soon as these temperatures have reached a steady state, the material in the barrel is pumped out. Second, the barrel temperature can be set to the required processing temperature or the heaters can be shut down.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.