Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® 1000 P - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® 1000 P:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Unreinforced, low-viscosity polyether ether ketone powder

VESTAKEEP® 1000 P is an unreinforced, low-viscosity polyether ether ketone powder. The product is suitable for the manufacture of compounds or it can be used as scatterpowder for the manufacture of composites.

The semi-crystalline polymer features superior thermal and chemical resistance.
Parts made from VESTAKEEP® 1000 P are of low flammability.

VESTAKEEP® 1000 P is supplied as a powder in boxes with moisture-proof polyethylene liners.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

Pigmentation may affect values.

For information about processing of VESTAKEEP® 1000 P, please follow the general recommendations in our brochure “VESTAKEEP® Polyether Ether Ketone.“

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.INDUSTRIAL.VESTAKEEP.COM
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 150 cm³/10min ISO 1133
Temperatura 380 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 3900 MPa ISO 527
Carico unitario a trazione 100 MPa ISO 527
Deformazione a snervamento 5.5 % ISO 527
Deformazione nominale a rottura 10 % ISO 527
Resistenza all'urto Charpy, +23°C 60 kJ/m² ISO 179/1eU
Type of failure C - -
Resistenza all'urto Charpy, -30°C 60 kJ/m² ISO 179/1eU
Type of failure C - -
Resistenzia all'urto Charpy con intaglio, +23°C 5 kJ/m² ISO 179/1eA
Type of failure C - -
Resistenzia all'urto Charpy con intaglio, -30°C 5 kJ/m² ISO 179/1eA
Type of failure C - -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 340 °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 150 °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 155 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 205 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 310 °C ISO 306
Reaz. al fuoco spess.nom. 1.5mm V-0 class IEC 60695-11-10
Spessore provato 1.6 mm -
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1300 kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 380 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 180 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Caratteristiche
Processabilità e Forma di Forni
Rivestimento, Stampaggio a Trasferimento
Forma fisica disponibile
Polveri
Caratteristiche
Stabilità termica
Resistenza Chimica
Resistenza chimica generale
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com