Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® 5000 G - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® 5000 G:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
High viscosity, unreinforced polyether ether ketone

VESTAKEEP® 5000 G is a high viscosity, unreinforced polyether ether ketone for injection molding and extrusion.

The semi-crystalline polymer features superior, thermal and chemical resistance. Parts made from VESTAKEEP® 5000 G are of low flammability.

VESTAKEEP® 5000 G can be processed by common machines for thermoplastics.
We recommend a melt temperature between 370°C and 380°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

VESTAKEEP® 5000 G is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

Pigmentation may affect values.

The results shown have been generated from a low number of production lots. Therefore, they are preliminary and not yet the result of a statistical evaluation. Therefore they must not be used to establish specifications.

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT WWW.INDUSTRIAL.VESTAKEEP.COM
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 7 cm³/10min ISO 1133
Temperatura 380 °C -
Carico 5 kg -
Ritiro di stampaggio, parallelo 0.9 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.1 % ISO 294-4, 2577
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 3500 MPa ISO 527
Carico unitario a trazione 95 MPa ISO 527
Deformazione a snervamento 5 % ISO 527
Deformazione nominale a rottura 35 % ISO 527
Resistenza all'urto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C N kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 9 kJ/m² ISO 179/1eA
Type of failure C - -
Resistenzia all'urto Charpy con intaglio, -30°C 8 kJ/m² ISO 179/1eA
Type of failure C - -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 340 °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 152 °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 150 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 205 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 305 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 60 E-6/K ISO 11359-1/-2
Indice di ossigeno 36 % ISO 4589-1/-2
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 2.8 - IEC 62631-2-1
Resistività volumica >1E13 Ohm*m IEC 62631-3-1
Rigidità dielettrica 32.9 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 200 - IEC 60112
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.5 % Sim. alla ISO 62
Assorbimento d'umidità 0.12 % Sim. alla ISO 62
Massa volumica 1300 kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 380 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 180 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Altre Estrusioni
Forma fisica disponibile
Pellet
Caratteristiche
Stabilità termica
Resistenza Chimica
Resistenza chimica generale
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.