Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® DC 4460 G - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® DC 4460 G:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
X-ray opaque, tooth-colored polyether ether ketone for dental applications

VESTAKEEP® DC4460 G is a tooth-colored, high viscosity polyether ether ketone (PEEK) resin that is especially designed for removable and fixed dentures, crowns and bridges.

VESTAKEEP® DC4460 G contains 6% Barium sulphate to render it x-ray opaque. 

Biocompatibility of VESTAKEEP® Dental
For VESTAKEEP® DC4460 G, biocompatibility has been tested according to ISO 10993-1 recommendations for permanent mucous membrane contact. The compound composition is optimised for high biocompatibility and superior mechanical, thermal and chemical resistance.
 
Biocompatibility test reports available for VESTAKEEP® DC4460 G
Standard Description
ISO 10993-03 Genotoxicity: Salmonella Typhimurium Reverse Mutation Test (Ames Test)
ISO 10993-05 Cytotoxicity: Quantitative Growth Inhibition Test
ISO 10993-10 Irritation: Intracutaneous Reactivity
ISO 10993-10 Sensitization: Local Lymph Node Assay
ISO 10993-11 Acute Systemic Toxicity
ISO 10993-11 Subacute / Subchronic Toxicity 14 days
ISO 10993-18 Extraction Tests
USP Class VI Acute Systemic Toxicity Intracutaneous Reactivity Muscle Implantation

Processing of VESTAKEEP® Dental
VESTAKEEP® DC4460 G can be processed by common melt processing techniques like injection molding and extrusion.
For injection molding, we recommend a melt temperature in the 380°C to 400°C range. The mold temperature should be within 160°C to 200°C, preferably 180°C.

Delivery of VESTAKEEP® Dental
VESTAKEEP® DC4460 G is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners.

The values presented are typical or average values, they do not constitute a specification. 
 
FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY 
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 10 cm³/10min ISO 1133
Temperatura 380 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 4100 MPa ISO 527
Carico unitario a trazione 95 MPa ISO 527
Deformazione a snervamento 4.8 % ISO 527
Resistenzia all'urto Charpy con intaglio, +23°C 6.8 kJ/m² ISO 179/1eA
Type of failure C - -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 340 °C ISO 11357-1/-3
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.4 % Sim. alla ISO 62
Massa volumica 1520 kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 400 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 180 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Altre Estrusioni
Forma fisica disponibile
Pellet
Resistenza Chimica
Resistenza chimica generale
Certifications
Biocompatibility ISO 10993, Approvazione della USP class VI
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.