Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9008 BK 9.7504 - PA12-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9008 BK 9.7504:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

High-viscosity, plasticizer-free extrusion compound with an extraordinary long-term heat resistance

VESTAMID® LX9008 BK 9.7504 is a plasticizer-free polyamide 12 compound, with an especially high long-term resistance under thermal load.

VESTAMID®  LX9008 BK 9.7504 is suitable to produce flexible tubes that are permanently exposed to higher temperatures, e.g., in the engine compartment of motor vehicles. Especially when used as diesel fuel lines they show significant advantages compared with standard grades, obvious in storage tests with diesel fuel.

The material absorbs only little moisture, thus leading to nearly unaffected dimensions and properties of the finished parts at changing ambient conditions.

Using VESTAMID® LX9008 BK 9.7504 for fuel lines one must pay attention to certain preconditions. The Technical Marketing Department gives you advice in selecting the suitable VESTAMID® compound.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 
 
FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.2 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.9 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 1450 / 970 MPa ISO 527
Carico unitario a trazione 41 / 39 MPa ISO 527
Deformazione a snervamento 5 / 17 % ISO 527
Deformazione nominale a rottura >50 / >50 % ISO 527
Resistenza all'urto Charpy, +23°C N / N kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 40 / 90 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 22 / 22 kJ/m² ISO 179/1eA
Type of failure C / C - -
Durezza Shore D 73 / * - ISO 7619-1
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 176 / * °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 47 / * °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 48 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 113 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 145 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 90.5 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 120 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3.7 / 4.7 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 2.9 / 3.1 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 520 / 1040 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 320 / 390 E-4 IEC 62631-2-1
Resistività volumica 1E12 / 2.3E10 Ohm*m IEC 62631-3-1
Rigidità dielettrica 38 / 37 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 600 / - - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 1.4 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.7 / * % Sim. alla ISO 62
Massa volumica 1010 / - kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Estrusione di tubi, Estrusione Profilati, Altre Estrusioni
Forma fisica disponibile
Pellet, Nero
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile al calore
Disponibilità geografica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.