Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9057 OR E20081 - PA12 FR(30+40) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9057 OR E20081:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Low-viscosity, self-extinguishing PA12 Compound, free of halogen, PA12 FR(30 40)

VESTAMID® LX9057 OR E20081 is a heat- stabilized compound with an efficient halogen-free flame retardant. Tested according to UL94, it complies with the flammability classification V-2.

The halogen-free formulation makes VESTAMID® LX9057 OR E20081 especially suitable for the electronic and cable industry.

VESTAMID® LX9057 OR E20081 can be used for injection molding as well as for wire extrusion coating.

The semi-crystalline compounds based on PA12 only absorb small amounts of water. Therefore manufactured parts exhibit excellent dimensional stability at changing ambient humidity, constant high toughness, low coefficient of friction and good chemical resistance.
  
Due to the presence of flame retardant the melt temperature should not exceed 240°C. We recommend melt temperatures of 200°C-220°C.
 
VESTAMID® LX9057 OR is supplied as cylindrical granules, ready for processing, in moisture-proof bags.
 
Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 45 / * cm³/10min ISO 1133
Temperatura 220 / * °C -
Carico 2.16 / * kg -
Ritiro di stampaggio, parallelo 0.9 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.0 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 1200 / 820 MPa ISO 527
Carico unitario a trazione 37 / 33 MPa ISO 527
Deformazione a snervamento 12 / 17 % ISO 527
Deformazione nominale a rottura >50 / >50 % ISO 527
Resistenza all'urto Charpy, +23°C 130 / N kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistenza all'urto Charpy, -30°C 69 / 122 kJ/m² ISO 179/1eU
Type of failure C / C - -
Resistenzia all'urto Charpy con intaglio, +23°C 3 / 7 kJ/m² ISO 179/1eA
Type of failure C / C - -
Resistenzia all'urto Charpy con intaglio, -30°C 3 / 2 kJ/m² ISO 179/1eA
Type of failure C / C - -
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 176 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 55 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 130 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 136 / * °C ISO 306
Reaz. al fuoco spess.nom. 1.5mm V-2 / * class IEC 60695-11-10
Spessore provato 1.5 / * mm -
Yellow Card disponibile sì / * - -
Reazione al fuoco a spessore h V-2 / * class IEC 60695-11-10
Spessore provato 0.8 / * mm -
Yellow Card disponibile sì / * - -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 4.5 / 7.5 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3.2 / 3.5 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 920 / 1920 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz - / 537 E-4 IEC 62631-2-1
Resistività volumica 7.4E11 / 9.3E9 Ohm*m IEC 62631-3-1
Rigidità dielettrica 35 / 36 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 600 / - - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 1.8 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.8 / * % Sim. alla ISO 62
Massa volumica 1080 / - kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Rivestimento
Forma fisica disponibile
Pellet
Caratteristiche speciali
Ritardante di fiamma, Senza alogeni, Stabilizzato o stabile al calore
Caratteristiche
Grado tribologico
Resistenza Chimica
Resistenza chimica generale
Applicazioni
Elettrotecnica ed electrici
Disponibilità geografica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.