Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® X7167 - PA12 FR(30) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® X7167:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

High viscosity, self-extinguishing PA12 compound, free of halogen and phosphorus

VESTAMID® X7167 NC is a heat stabilized PA12 compound containing a non-migrating flame retardant, free of halogen and phosphorous.
 

VESTAMID® X7167 NC complies with the requirements of FAR 25.853 or ABD 0031. The absence of halogens and phosphorous makes VESTAMID® X7167 NC especially suitable for interior parts in aircrafts, railways and ships.
 

This resin can be used for extrusion as well as for injection molding. Due to the presence of flame retardant melt temperature should not exceed 260 °C. We recommend melt temperatures of 210 - 230 °C.
 

VESTAMID® X7167 NC is supplied as cylindrical pellets, ready for use, in moisture-proof bags.

The use of colorants may affect property values. 


Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.


For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 


The values presented are typical or average values, they do not constitute a specification.


FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 4.1 / * cm³/10min ISO 1133
Temperatura 230 / * °C -
Carico 2.16 / * kg -
Ritiro di stampaggio, parallelo 0.6 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.9 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 1700 / 1440 MPa ISO 527
Carico unitario a trazione 47 / 42 MPa ISO 527
Deformazione a snervamento 5 / 13 % ISO 527
Deformazione nominale a rottura >50 / >50 % ISO 527
Resistenza all'urto Charpy, +23°C N / N kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 7 / 9 kJ/m² ISO 179/1eA
Type of failure C / C - -
Resistenzia all'urto Charpy con intaglio, -30°C 6 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 178 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 50 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 130 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 150 / * °C ISO 306
Reaz. al fuoco spess.nom. 1.5mm V-2 / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Indice di ossigeno 26 / * % ISO 4589-1/-2
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz - / 4.8 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3.6 / 3.2 - IEC 62631-2-1
Fattore di dissipazione, 100Hz - / 800 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 380 / 400 E-4 IEC 62631-2-1
Resistività volumica 1E12 / 2E12 Ohm*m IEC 62631-3-1
Rigidità dielettrica 34 / 36 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 600 / - - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 1.5 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.6 / * % Sim. alla ISO 62
Massa volumica 1050 / - kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 240 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 80 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Stamp. ad Iniezione, pressione di chiusura 70 MPa ISO 294
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione Profilati, Altre Estrusioni
Forma fisica disponibile
Pellet, Colore naturale
Additivi
Lubrificanti
Caratteristiche speciali
Ritardante di fiamma, Senza alogeni, Senza fosforo, Stabilizzato o stabile al calore
Applicazioni
Aereo e aerospaziale
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.