Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® X7297 BK 9.7507 - PA12-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® X7297 BK 9.7507:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
High viscosity, plasticized, impact-modified, heat- and light stabilized PA 12 compound

VESTAMID® X7297 BK 9.7507 is a plasticized polyamide 12 compound with heat and light stabilizer for the extrusion of flexible tubing and hose especially for automotive applications.

 

VESTAMID® X7297 BK 9.7507 is characterized by easy processing as well as high impact strength at low temperatures.

 

Properties of compounds based on polyamide 12 vary little with changing humidity due to low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance.
 

VESTAMID® X7297 BK 9.7507 is supplied as cylindrical pellets, ready for processing, in moisture-proof bags.

The use of colorants may affect property values. 
  
Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 13 / * cm³/10min ISO 1133
Temperatura 230 / * °C -
Carico 5 / * kg -
Ritiro di stampaggio, parallelo 0.9 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.3 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 390 / 390 MPa ISO 527
Carico unitario a trazione 26 / 25 MPa ISO 527
Deformazione a snervamento 37 / 37 % ISO 527
Deformazione nominale a rottura >50 / >50 % ISO 527
Resistenza all'urto Charpy, +23°C N / N kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 122 / 130 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 6 / 8 kJ/m² ISO 179/1eA
Type of failure C / C - -
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 171 / * °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 41 / * °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 51 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 135 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 125 / * °C ISO 306
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 11.4 / 13.7 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3.6 / 3.8 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 1850 / 2260 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 1040 / 1570 E-4 IEC 62631-2-1
Resistività volumica 3.3E9 / 6.3E8 Ohm*m IEC 62631-3-1
Rigidità dielettrica 36 / 36 kV/mm IEC 60243-1
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 1.4 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.8 / * % Sim. alla ISO 62
Massa volumica 1020 / - kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 220 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 60 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Caratteristiche
Processabilità e Forma di Forni
Estrusione di tubi, Altre Estrusioni
Forma fisica disponibile
Pellet, Nero
Additivi
Plastificante
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile alla luce, Estab. agli U.V. o per applicaz.in esterni, Stabilizzato o stabile al calore
Caratteristiche
Grado tribologico
Resistenza Chimica
Resistenza chimica generale
Applicazioni
Automotive
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.