Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTORAN® X7342 - PPE-GF20 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTORAN® X7342:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestoran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Modified polyphenylene ether (PPE), high heat resistant, 20 % glass fiber-reinforced

VESTORAN® X7342 is the registered trademark of the Evonik Degussa GmbH for molding compounds containing poly-2,6-dimethyl-1,4-phenylene ether as polymeric constituent (poly-phenylene ether, PPE, also referred to as PPO).

As a material of amorphous structure, VESTORAN® X7342 shows very small mold shrinkage. Therefore molded parts have a very low tendency to warp.

Moldings of VESTORAN® X7342 are dimen­sionally stable and hydrolysis resistant even in hot water, but are more sensitive to organic solvents than semi-crystalline plastics. VESTORAN® X7342 is resistant to aqueous alkalines and acides, certain alcohols, and glycol solutions.

Due to the glass fiber-reinforcement the compound combines outstanding heat deflection temperature under load with high strength and rigidity. The even smaller shrinkage compared to non-reinforced VESTORAN® depends on the orientation of the glass fibers in the molded part.
 
VESTORAN® X7342 is supplied as cylindrical granules in polyethylene packaging.
 
Processing advice is given in a separate product information.

Pigmentation may affect values.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 40 cm³/10min ISO 1133
Temperatura 300 °C -
Carico 21.6 kg -
Ritiro di stampaggio, parallelo 0.2 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.4 % ISO 294-4, 2577
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 6100 MPa ISO 527
Carico unitario a rottura 108 MPa ISO 527
Deformazione a rottura 3.5 % ISO 527
Resistenza all'urto Charpy, +23°C 49 kJ/m² ISO 179/1eU
Type of failure C - -
Resistenzia all'urto Charpy con intaglio, +23°C 13 kJ/m² ISO 179/1eA
Type of failure C - -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 165 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 170 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 170 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 40 E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 30 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.6 mm -
Reazione al fuoco a spessore h HB class IEC 60695-11-10
Spessore provato 0.8 mm -
Yellow Card disponibile - -
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3.5 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 80 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 10 E-4 IEC 62631-2-1
Resistività volumica 1E11 Ohm*m IEC 62631-3-1
Res. Alle correnti striscianti superficiali 175 - IEC 60112
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1190 kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Caratteristiche speciali
Stabilizzato o stabile al calore
Caratteristiche
Amorfo, Bassa deformazione
Resistenza Chimica
Resistenza all'acido, Resistenza agli alcali, Stabilità idrolitica
Disponibilità geografica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.