Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of iOn™ Nylon 6 Copolymer - PA6 - 3DXTECH

Material Data Center offers the following functions for iOn™ Nylon 6 Copolymer:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other iOn datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Limited resistance. Considerable dimensional changes, and possibly
irreversible changes in properties after prolonged contact. Consultation
advisable before use.

Please consider the information about the application of the materials.
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di transizione vetrosa, 10°C/min 105 °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 97 °C ISO 75-1/-2
Proprietà ElettricheValoreUnitáNorma del test
ASTM Data
Resistenza superficiale 1E13 Ohm ASTM D 257
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1060 kg/m³ ISO 1183
3D DataValoreUnitáNorma del test
Modulo a trazione, flat 2090[1] MPa -
Carico unitario a rottura, flat 45[1] MPa -
Deformazione a rottura, flat 8[1] % -
Modulo a flessione, flat 2210[1] MPa -
Resistenza alla flessione, flat 80[1] MPa -
1: 45°-45°
Caratteristiche
Processabilità e Forma di Forni
Additive Manufacturing
Forma fisica disponibile
Monofilament, Colore naturale
Caratteristiche
Copolimero
Disponibilità geografica
Nord America, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.