Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Bio-Flex® F 6510 - (PLA+Copolyester) - FKuR Kunststoff GmbH

Material Data Center offers the following functions for Bio-Flex® F 6510:
unit conversion, PDF datasheet print, application examples, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Bio-Flex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 2.7 cm³/10min ISO 1133
温度 190 °C -
荷重 2.16 kg -
メルトフローレート, MFI 3.2 g/10min ISO 1133
温度 190 °C -
荷重 2.16 kg -
成形収縮率, 平行 0.3 % ISO 294-4, 2577
成形収縮率, 直角 0.3 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 2600 MPa ISO 527
引張強度 47 MPa ISO 527
降伏ひずみ 4 % ISO 527
破壊応力 23 MPa ISO 527
破壊ひずみ 19 % ISO 527
曲げ弾性率, 23°C 2650 MPa ISO 178
シャルピー衝撃強さ, +23°C N kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 7 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
溶融温度, 10゚C/min 155 °C ISO 11357-1/-3
ビカット軟化温度, A 60 °C ISO 306
その他の特性.単位テスト基準
密度. 1300 kg/m³ ISO 1183
Biobased content 70 % -
機械的特性(ィルム)単位テスト基準
ISO データ
水蒸気透過度, 23°C/85%r.h. 130 g/(m²*d) ISO 15106-1/-2
試験片の厚さ. 0.02 mm -
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 60 °C -
Pre-drying - Time 2 - 4 h -
樹脂温度 195 °C -
金型温度 40 °C -
Feed temperature 45 °C -
Zone 1 150 °C -
Zone 2 160 °C -
Zone 3 180 °C -
Nozzle temperature 190 °C -
Injection pressure 200 MPa -
Back pressure 3 - 8 MPa -
特殊な特性
成形加工法.
射出成形., フィルム押出成形.
納入形状.
ペレット., 白
Certifications
Contains renewable resources, Biodegradable, Food contact, 堆肥化可能 ISO 13432 (プロデューサー), 堆肥化可能 ISO 13432 (証明書)
アプリケーション
パッケージング, おもちゃ
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.