Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Bio-Flex® S 5514 - PLA... - FKuR Kunststoff GmbH

Material Data Center offers the following functions for Bio-Flex® S 5514:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Bio-Flex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
more information can be found in the following table
Rilsamid® Chemical Resistance
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 25 g/10min ISO 1133
温度 190 °C -
荷重 2.16 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 2550 MPa ISO 527
引張強度 43 MPa ISO 527
降伏ひずみ 5 % ISO 527
破壊応力 20 MPa ISO 527
破壊ひずみ 13.5 % ISO 527
シャルピー衝撃強さ, +23°C 43 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 3.5 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
溶融温度, 10゚C/min 155 °C ISO 11357-1/-3
荷重たわみ温度, 0.45 MPa 59 °C ISO 75-1/-2
ビカット軟化温度, A 110 °C ISO 306
その他の特性.単位テスト基準
密度. 1370 kg/m³ ISO 1183
Biobased content 75 % -
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 60 °C -
Pre-drying - Time 2 - 4 h -
金型温度 30 - 60 °C -
Feed temperature 60 °C -
Zone 1 160 °C -
Zone 2 170 °C -
Zone 3 180 °C -
Nozzle temperature 190 °C -
Maximum residence time 5 min -
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
Certifications
Contains renewable resources, Biodegradable, 堆肥化可能 ISO 13432 (プロデューサー), 堆肥化可能 ISO 13432 (証明書)
アプリケーション
おもちゃ
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.