Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cadence™ GS3 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Cadence™ GS3:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Cadence datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Eastman Cadence™ GS3 is a clear copolyester resin specifically for calendered film applications including

decorative laminates, general purpose packaging, transaction and identification cards, and protective films. It has

enhanced processing ease and higher melt strength compared to Cadence™ GS2.

Film producers looking to replace PVC and other materials of concern choose Cadence™ for its ease of processing,

low-temperature toughness, and the ability to be downgauged – all of which help reduce cost. It has a wide

calendering and thermoforming window, which enables Cadence™ to be used on most existing calendering lines

and thermoforming equipment with little or no modification. Eastman Cadence™ resins require no pre-drying or

additional stabilizers.

熱的特性単位テスト基準
ASTM数据
線膨張係数, 平行 75.2 E-6/K ASTM D 696
DTUL @ 66 psi 69 °C ASTM D 648
DTUL @ 264 psi 62 °C ASTM D 648
ガラス転移温度 80 °C ASTM E 1356
ビカット軟化温度 81 °C ASTM D 1525
酸素指数 24.2 % ASTM D 2863
電気的特性.単位テスト基準
ASTM数据
耐電圧, 短い時間 15.1 kV/mm ASTM D 149
誘電正接, 1 MHz 0.019 - ASTM D 150
比誘電率, 1 MHz 2.43 - ASTM D 150
表面抵抗率 1.28E16 Ohm ASTM D 257
体積抵抗率 7.05E16 Ohm*cm ASTM D 257
耐アーク 135 s ASTM D 495
その他の特性.単位テスト基準
吸水率, 24hr 0.15 % ASTM D 570
密度 1280 kg/m³ ASTM D 792
特殊な特性
成形加工法.
カレンダー加工., 熱成形.
な特性
Low Emission, Melt Strength, Scratch Resistant, Copolymer
Certifications
Food contact, Food approval FDA 21 CFR
アプリケーション
建築構造, パッケージング
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.