Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CALIBRE™ 5201-12 - PC-GX20 - Trinseo

Material Data Center offers the following functions for CALIBRE™ 5201-12:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Calibre datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 12 g/10min ISO 1133
温度 300 °C -
荷重 1.2 kg -
成形収縮率, 平行 0.3 % ISO 294-4, 2577
ASTM数据
メルトフローレイト, MFI 12 g/10min ASTM D 1238
温度 300 °C -
荷重 1.2 kg -
成形収縮率., 平行 0.003 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張弾性率 5170 MPa ISO 527
降伏応力 82.7 MPa ISO 527
降伏ひずみ 2.6 % ISO 527
破壊応力 82.7 MPa ISO 527
破壊ひずみ 2.6 % ISO 527
曲げ弾性率, 23°C 4820 MPa ISO 178
ASTM数据
引張弾性率 5171 MPa ASTM D 638
降伏応力 8.27 MPa ASTM D 638
破壊応力 8.27 MPa ASTM D 638
降伏点伸び 2.6 % ASTM D 638
破断伸び 3 % ASTM D 638
曲げ弾性率 4826 MPa ASTM D 790
曲げ強さ 148 MPa ASTM D 790
ロックウェル硬度 R 122 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 107 J/m ASTM D 256
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 138 °C ISO 75-1/-2
ビカット軟化温度, B 158 °C ISO 306
1.5mm厚さでの燃焼性 V-2 class IEC 60695-11-10
試験片の厚さ 1.6 mm -
厚さhでの燃焼性 V-0 class IEC 60695-11-10
試験片の厚さ 3.0 mm -
ASTM数据
UL94 燃焼性 V-2 - UL 94
追加試験片の厚さ 1.59 mm -
DTUL @ 264 psi 138 °C ASTM D 648
ビカット軟化温度 159 °C ASTM D 1525
その他の特性.単位テスト基準
密度. 1360 kg/m³ ISO 1183
密度 1360 kg/m³ ASTM D 792
特殊な特性
アプリケーション
電気電子, 医療の
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.