Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cawiton MT960 - SEBS - Wittenburg B.V.

Material Data Center offers the following functions for Cawiton MT960:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Cawiton datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 5.6 g/10min ISO 1133
温度 230 °C -
荷重 5 kg -
機械的特性単位テスト基準
ISO データ
引張強度 3.8 MPa ISO 37
破壊ひずみ 303 % ISO 37
圧縮永久ひずみ 70℃, 24h 51 % ISO 815
引裂強さ 29.5 kN/m ISO 34-1
ショア硬さA 60 - ISO 7619-1
Other Standards[S]
伸び率100%時の応力 2.7 MPa ISO 37
伸び率300%時の応力 9.9 MPa ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
熱的特性単位テスト基準
ISO データ
溶融温度, 10゚C/min 166 °C ISO 11357-1/-3
その他の特性.単位テスト基準
密度. 900 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
樹脂温度 180 - 240 °C -
金型温度 20 - 40 °C -
Feed temperature 30 - 60 °C -
Zone 1 180 - 220 °C -
Zone 2 190 - 230 °C -
Zone 3 190 - 230 °C -
Nozzle temperature 200 - 240 °C -
特殊な特性
成形加工法.
射出成形.
特殊な特性.
Translucent, 滅菌可能, エチレンオキシド滅菌(EtO), 蒸気滅菌, Gamma irradiation sterilization
耐薬品性
Radiation Resistance
Certifications
Food contact, Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
アプリケーション
医療の
領域別の利用可能性
ヨーロッパ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.