Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELSTRAN® PP-GF50-0453 P10/10 - PP-GLF50 - Celanese

Material Data Center offers the following functions for CELSTRAN® PP-GF50-0453 P10/10:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Celstran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Material code according to ISO 1043-1: PP Heat stabilized polypropylene reinforced with 50 weight percent long glass fibers. Black. The product has low emissions. The fibers are chemically coupled to the polypropylene matrix. The pellets are cylindrical and normally as well as the embedded fibers 11 mm long. Parts molded of CELSTRAN have outstanding mechanical properties such as high strength and stiffness combined with high heat deflection. The notched impact strength is increased at elevated and low temperatures due to the fiber skeleton built in the parts. The long fiber reinforcement reduces creep significantly. The very isotropic shrinkage in the molded parts minimizes the warpage. Complex parts can be manufactured with high reproducibility by injection molding. Application field: Functional/structural parts for automotive

Flammability at thickness h (1 mm)HB-
機械的特性単位テスト基準
ISO データ
引張弾性率 11600 MPa ISO 527
破壊応力 140 MPa ISO 527
破壊ひずみ 1.8 % ISO 527
シャルピー衝撃強さ, +23°C 60 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 58 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 32 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 33 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 166 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 158 °C ISO 75-1/-2
荷重たわみ温度, 8.00 MPa 134 °C ISO 75-1/-2
厚さhでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.0 mm -
その他の特性.単位テスト基準
密度 1340 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 94 °C -
Pre-drying - Time 2 h -
樹脂温度 260 - 290 °C -
金型温度 40 - 70 °C -
機能
 応力-ひずみ. , CELSTRAN® PP-GF50-0453 P10/10, PP-GLF50, Celanese
 割線弾性率−ひずみ. , CELSTRAN® PP-GF50-0453 P10/10, PP-GLF50, Celanese
特殊な特性
成形加工法.
射出成形., 異形押出成形., シート押出成形., その他の押出成形., コーティング., トランスファー成形.
納入形状.
ペレット., 黒
特殊な特性.
熱安定化.
な特性
Chemically Coupled Reinforcement, Creep Resistance, Long fiber reinforced, Low Emission, Low Warpage
アプリケーション
自動車
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域.
その他の情報
村遜速揃
PP&PE drying requirements: 2 hrs. @94° C.
A dehumidifier or desiccant dryer is recommended.
Celstran can be processed on a standard injection molding unit.
A general purpose metering screw is recommended with a zone
distribution of 40% feed, 40% transition, and 20% metering.
A free flowing check ring assembly is recommended.

Melt Temp: 230-240°C.
Mold Temp: 30- 70°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.