Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cristal™ Renew 400-50 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Cristal™ Renew 400-50:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Cristal datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Eastman Cristal™ Renew copolyester 400-50 is a high flow product. It is designed and engineered specifically for

cosmetics packaging applications. With its unsurpassed color and clarity and an unmatched ability to mold thick

parts with improved gate aesthetics, Cristal Renew 400-50 is clearly a well suited copolyester for premium

cosmetics packaging. Other outstanding features are excellent chemical resistance, high gloss, and improvements

in processing such as faster cycle times, and lower scrap rates. Cristal Renew 400-50 is also ideally suited for twoshot

molding techniques due to its lower processing temperatures, very slow crystallization rate, and flow

characteristics.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a

global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are

produced with ISCC certified circular content by mass balance allocation.


Processing/Physical Characteristics単位テスト基準
ASTM数据
成形収縮率., 平行 0.0035 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張弾性率 2000 MPa ISO 527
降伏応力 49 MPa ISO 527
降伏ひずみ 4.2 % ISO 527
破壊応力 21 MPa ISO 527
破壊ひずみ 36 % ISO 527
ASTM数据
引張弾性率 2030 MPa ASTM D 638
降伏応力 50 MPa ASTM D 638
破壊応力 25 MPa ASTM D 638
降伏点伸び 4.4 % ASTM D 638
破断伸び 38 % ASTM D 638
曲げ弾性率 1810 MPa ASTM D 790
曲げ強さ 66 MPa ASTM D 790
ロックウェル硬度 R 102 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 104 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 38 J/m ASTM D 256
温度 -40 °C -
アイゾット衝撃試験, 1/8 in N J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
DTUL @ 66 psi 68 °C ASTM D 648
DTUL @ 264 psi 61 °C ASTM D 648
光学特性単位テスト基準
ASTM数据
ヘイズ 0.24 % ASTM D 1003
視感透過率 91.8 % ASTM D 1003
その他の特性.単位テスト基準
密度 1280 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 65 °C -
Pre-drying - Time 8 h -
樹脂温度 205 - 240 °C -
金型温度 16 - 38 °C -
特殊な特性
成形加工法.
射出成形., その他の押出成形.
特殊な特性.
高耐衝撃及び耐衝撃改良., 透明.
な特性
High Gloss, Copolymer
耐薬品性
General Chemical Resistance
Certifications
ISCC Plus
アプリケーション
パッケージング
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.