Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delas 180 - (NBR+PVC) - Lingen Plastic Rubber Co., Ltd.

Material Data Center offers the following functions for Delas 180:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Delas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
機械的特性単位テスト基準
ASTM数据
ショア硬さA 80 - ASTM D 2240
引裂強さ 38 kN/m ASTM D 624
圧縮永久ひずみ, 22 hr @ 158 °F 64 % ASTM D 395
引張強度 11.7 MPa ASTM D 412
その他の特性.単位テスト基準
密度 1270 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 60 °C -
Pre-drying - Time 4 - 6 h -
樹脂温度 170 °C -
金型温度 30 - 80 °C -
Zone 1 130 - 140 °C -
Zone 2 140 - 160 °C -
Zone 3 160 - 190 °C -
Nozzle temperature 170 - 190 °C -
Screw speed 100 - 200 rpm -
Back pressure 0.05 - 0.5 MPa -
Processing Recommendation Extrusion単位テスト基準
Pre-drying - Temperature 60 °C -
Pre-drying - Time 4 - 6 h -
樹脂温度 160 °C -
金型温度 150 - 170 °C -
Feed temperature 130 - 140 °C -
Zone 1 140 - 150 °C -
Zone 2 140 - 150 °C -
Zone 3 150 - 170 °C -
特殊な特性
成形加工法.
射出成形., その他の押出成形.
特殊な特性.
紫外線安定化.
耐薬品性
Grease Resistance
領域別の利用可能性
アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.