Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of DuraStar™ DS2000 - PCTA - Eastman Chemical Co.

Material Data Center offers the following functions for DuraStar™ DS2000:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Durastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Durastar™ DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has very good toughness as shown by Izod impact resistance. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but DS2000 maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged. Easy to process, it flows readily and fills intricate molds. Under existing United States Food and Drug Administration (FDA) regulations, Durastar™ DS2000 may be used in food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240.




Processing/Physical Characteristics単位テスト基準
ASTM数据
成形収縮率., 平行 0.004 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
降伏応力 47 MPa ISO 527
降伏ひずみ 4 % ISO 527
破壊応力 49 MPa ISO 527
破壊ひずみ 210 % ISO 527
曲げ弾性率, 23°C 1750 MPa ISO 178
曲げ強さ 64 MPa ISO 178
ノッチ付きIzod衝撃強さ, +23°C 29.6 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ 6.3 kJ/m² ISO 180/1A
温度 -40 °C -
パンクチャー衝撃エネルギー, +23゚C 71 J ISO 6603-2
ASTM数据
降伏応力 46 MPa ASTM D 638
破壊応力 53.1 MPa ASTM D 638
降伏点伸び 5 % ASTM D 638
破断伸び 310 % ASTM D 638
曲げ弾性率 1900 MPa ASTM D 790
ロックウェル硬度 105 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 370 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 60 J/m ASTM D 256
温度 -40 °C -
アイゾット衝撃試験, 1/8 in N J/m ASTM D 256
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 66 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 73 °C ISO 75-1/-2
ASTM数据
UL94 燃焼性 HB - UL 94
追加試験片の厚さ 1.5 mm -
DTUL @ 66 psi 73 °C ASTM D 648
DTUL @ 264 psi 65 °C ASTM D 648
光学特性単位テスト基準
ASTM数据
ヘイズ 0.3 % ASTM D 1003
視感透過率 91 % ASTM D 1003
その他の特性.単位テスト基準
密度. 1190 kg/m³ ISO 1183
密度 1200 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 70 °C -
Pre-drying - Time 3 h -
樹脂温度 250 - 290 °C -
金型温度 15 - 30 °C -
特殊な特性
成形加工法.
射出成形.
納入形状.
ナチュラルカラー
特殊な特性.
高耐衝撃及び耐衝撃改良., 透明.
耐薬品性
General Chemical Resistance, Oil Resistance
Certifications
Food contact, Food approval FDA 21 CFR
アプリケーション
建築構造, スポーツ用品
領域別の利用可能性
ヨーロッパ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.