Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Dynaflex™ G2706-1000-00 - TPE - Avient Corporation

Material Data Center offers the following functions for Dynaflex™ G2706-1000-00:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Dynaflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 1 g/10min ASTM D 1238
温度 200 °C -
荷重 5 kg -
成形収縮率., 平行 0.05 mm/mm ASTM D 955
機械的特性単位テスト基準
ASTM数据
伸び率100%弾性率 0.621 MPa ASTM D 412
伸び率300%弾性率 0.63 MPa ASTM D 412
ショア硬さA 28 - ASTM D 2240
引裂強さ 14 kN/m ASTM D 624
圧縮永久ひずみ, 22 hr @ 73 °F 8 % ASTM D 395
破壊応力 5.52 MPa ASTM D 412
破断伸び 660 % ASTM D 412
その他の特性.単位テスト基準
密度 890 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
金型温度 15.6 - 37.8 °C -
Zone 1 160 - 199 °C -
Zone 2 171 - 210 °C -
Zone 3 188 - 227 °C -
Nozzle temperature 188 - 227 °C -
Screw speed 25 - 75 rpm -
Injection speed 25.4 - 127 mm/s -
Back pressure 0 - 0.758 MPa -
後硬化時間 0.931 - 2.07 MPa -
特殊な特性
成形加工法.
射出成形., その他の押出成形.
納入形状.
ペレット.
特殊な特性.
透明.
な特性
Good Adhesion, Soft Feel
Certifications
Food contact, Food approval 10/2011, Food approval FDA 21 CFR, US Pharmacopeia Class VI Approved
アプリケーション
自動車, 医療の
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.