Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Dynalloy™ OBC 8100-N50 - TPE - Avient Corporation

Material Data Center offers the following functions for Dynalloy™ OBC 8100-N50:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Dynalloy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
機械的特性単位テスト基準
ASTM数据
伸び率100%弾性率 1.48 MPa ASTM D 412
伸び率300%弾性率 0.63 MPa ASTM D 412
ショア硬さA 48 - ASTM D 2240
引裂強さ 17.5 kN/m ASTM D 624
破壊応力 3.31 MPa ASTM D 412
破断伸び 990 % ASTM D 412
その他の特性.単位テスト基準
密度 1060 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
金型温度 15.6 - 26.7 °C -
Zone 1 160 - 188 °C -
Zone 2 177 - 193 °C -
Zone 3 182 - 210 °C -
Nozzle temperature 193 - 216 °C -
Screw speed 25 - 100 rpm -
Injection speed 25.4 - 76.2 mm/s -
Back pressure 0 - 0.689 MPa -
後硬化時間 0.362 - 1.65 MPa -
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット., ナチュラルカラー
な特性
Good Adhesion, Soft Feel
Certifications
Food contact, Food approval BfR, Food approval FDA 21 CFR
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com