Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ CN015-50 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ CN015-50:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Eastar™ Renew CN015-50 Natural copolyester is a high flow product that contains a mold release to provide ease of demolding. Designed specifically for the unique requirements of luxury cosmetic packaging, our premier PCTA copolyester delivers unsurpassed color and clarity and a capability to mold thick parts with improved gate

aesthetics. Other outstanding features of Eastar™ Renew CN015-50 Natural copolyester include excellent chemical resistance, high gloss, and process enhancements such as faster drying times, faster cycle times, and lower scrap

rates. Eastar™ Renew CN015-50 Natural copolyester is also ideally suited for two-shot molding techniques due to its lower processing temperatures, very slow crystallization rate, and flow characteristics.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation. Renew polymers enable a brand to

reduce consumption of fossil feedstock-based plastics, achieve sustainability targets without compromise, and be a fast mover in a growing market for sustainable consumer products.

Processing/Physical Characteristics単位テスト基準
ASTM数据
成形収縮率., 平行 0.003 mm/mm ASTM D 955
機械的特性単位テスト基準
ASTM数据
降伏応力 50 MPa ASTM D 638
破壊応力 35 MPa ASTM D 638
降伏点伸び 4.5 % ASTM D 638
破断伸び 193 % ASTM D 638
曲げ弾性率 1800 MPa ASTM D 790
曲げ強さ 67 MPa ASTM D 790
ロックウェル硬度 R 105 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 70 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 38 J/m ASTM D 256
温度 -40 °C -
アイゾット衝撃試験, 1/8 in N J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
DTUL @ 66 psi 71 °C ASTM D 648
DTUL @ 264 psi 63 °C ASTM D 648
光学特性単位テスト基準
ASTM数据
ヘイズ 0.6 % ASTM D 1003
視感透過率 90 % ASTM D 1003
その他の特性.単位テスト基準
密度 1200 kg/m³ ASTM D 792
Processing Recommendation Extrusion単位テスト基準
Pre-drying - Temperature 60 °C -
Pre-drying - Time 2 - 4 h -
樹脂温度 225 - 245 °C -
金型温度 16 - 50 °C -
特殊な特性
成形加工法.
その他の押出成形.
納入形状.
ナチュラルカラー
添加剤.
離型剤.
特殊な特性.
高耐衝撃及び耐衝撃改良., 透明.
な特性
Heat Sealable, High Gloss, Copolymer
耐薬品性
General Chemical Resistance
Certifications
ISCC Plus
アプリケーション
パッケージング
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com