Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ EN052 - Polyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ EN052:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Eastar™ Polyester EN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystallized.





Processing/Physical Characteristics単位テスト基準
ASTM数据
成形収縮率., 平行 0.004 mm/mm ASTM D 955
機械的特性単位テスト基準
ASTM数据
降伏応力 57 MPa ASTM D 638
破壊応力 26 MPa ASTM D 638
降伏点伸び 4 % ASTM D 638
曲げ弾性率 2500 MPa ASTM D 790
ロックウェル硬度 R 110 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 51 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 36 J/m ASTM D 256
温度 -40 °C -
アイゾット衝撃試験, 1/8 in N J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
DTUL @ 66 psi 66 °C ASTM D 648
DTUL @ 264 psi 62 °C ASTM D 648
ビカット軟化温度 79 °C ASTM D 1525
電気的特性.単位テスト基準
ASTM数据
耐電圧, 短い時間 15.7 kV/mm ASTM D 149
誘電正接, 1 MHz 0.02 - ASTM D 150
比誘電率, 1 MHz 3 - ASTM D 150
表面抵抗率 1E16 Ohm ASTM D 257
体積抵抗率 1E16 Ohm*cm ASTM D 257
耐アーク 155 s ASTM D 495
その他の特性.単位テスト基準
吸水率, 24hr 0.1 % ASTM D 570
密度 1320 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 150 - 160 °C -
Pre-drying - Time 4 - 6 h -
樹脂温度 275 - 295 °C -
金型温度 10 - 30 °C -
特殊な特性
成形加工法.
射出成形.
な特性
Homopolymer
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com