Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ EN076 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ EN076:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Eastar™ EN076 copolyester is a clear copolyester used in a variety of packaging and consumer product applications, including food and beverage packaging, general purpose packaging, flexible film packaging, and consumer products. It is fully compatible with the resin identification code 1 (RIC1) recycle stream. Eastar EN076

enables fast-moving consumer-goods brand owners to achieve recyclable products and packaging and replace materials of concern without sacrificing aesthetics.


Eastar EN076 meets the definition of resin identification code PREPROCESSING (RIC1) as defined by ASTM D7611. Other endproduct attributes, including but not limited to size, color, auxiliary components, and availability of collection, may also impact recyclability.


Eastar EN076 copolyester may be used in various food contact applications under the U.S. Food & Drug Administration (FDA) regulations.




Processing/Physical Characteristics単位テスト基準
ASTM数据
成形収縮率., 平行 0.0035 mm/mm ASTM D 955
機械的特性単位テスト基準
ASTM数据
降伏応力 56 MPa ASTM D 638
破壊応力 26 MPa ASTM D 638
降伏点伸び 4 % ASTM D 638
破断伸び 75 % ASTM D 638
曲げ弾性率 2350 MPa ASTM D 790
ロックウェル硬度 111 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 67 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 33 J/m ASTM D 256
温度 -40 °C -
アイゾット衝撃試験, 1/8 in N J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
DTUL @ 66 psi 69 °C ASTM D 648
DTUL @ 264 psi 62 °C ASTM D 648
光学特性単位テスト基準
ASTM数据
ヘイズ 0.8 % ASTM D 1003
視感透過率 89 % ASTM D 1003
その他の特性.単位テスト基準
密度 1320 kg/m³ ASTM D 792
Processing Recommendation Extrusion単位テスト基準
Pre-drying - Temperature 150 °C -
Pre-drying - Time 4 - 6 h -
樹脂温度 277 - 293 °C -
金型温度 16 - 32 °C -
特殊な特性
成形加工法.
射出成形., フィルム押出成形., その他の押出成形., 熱成形.
な特性
Copolymer
Certifications
Food contact, Food approval FDA 21 CFR
アプリケーション
パッケージング
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.